| Ni粘结的Ti(C,N)金属陶瓷的横向断裂强度与断口的分形分析 |
| 刘宁;赵兴中;江来珠;罗会国;胡镇华;崔崑 |
| 华中理工大学;安徽工学院材料系 |
|
| TRANSVERSE RUPTURE STRENGTH OF Ni BONDED Ti(C, N) CERMET AND FRACTAL DIMENSION ANALYSIS OF ITS FRACTURE SURFACES |
| LIU Ning; ZHAO Hingzhong; JIANG Laizhu; LUO Huiguo; HU Zhenhua; CUI Kun(Huazhong University of Science and Technology; Wuhan 430074) |
引用本文:
刘宁;赵兴中;江来珠;罗会国;胡镇华;崔崑. Ni粘结的Ti(C,N)金属陶瓷的横向断裂强度与断口的分形分析[J]. 金属学报, 1995, 31(5): 229-235.
,
,
,
,
,
.
TRANSVERSE RUPTURE STRENGTH OF Ni BONDED Ti(C, N) CERMET AND FRACTAL DIMENSION ANALYSIS OF ITS FRACTURE SURFACES[J]. Acta Metall Sin, 1995, 31(5): 229-235.
| 1MandelbrotBB,PassojaDE,PaullayAJ.Nature,1984;308(5961):7212苏辉,张玉贵,阎振.金属学报,1989;25:A4663PandeCS,RichardsLE,LouatN,DempseyBD,SchwoebleAJ.ActaMetall,1987;35:16334UnderwoodEE,BanerjiK.MaterSciEng,1986,80(1):15LungCW,MuZQ.PhysRev,1988;B38:117816RichardsLE,DempseyBD.ScrMetall,1988;22:6877WangZG,ChenDL,JiangXX,AiSH,ShihCH.ScrMetall,1988;22:8278 ManddbrotBB,VannessJW.SoeInd ApplMathRey,1968;10:4229PentlandAP.IEEETrans,1984;PAMI-6(6):66110刘宁.华中理工大学博士学位论文,199411LungCW.In:PietroneroL,TosattiEeds.,FractalsinPhysics,North-Holland:ElsevierSciencePublishers.1986:18912谢和平,陈至达.力学学报,1988,20:26413 苏辉,陈冷,阎振.科学通报,1991;36:151014刘曼朗,黄孝瑛,段石田,邵大琴,崔玉梅,姚振海,金属学报,1982:18:68915 GoknhaleAM.MetallTrans,1990;21A:119316FalconerK著,曾文曲,刘世耀译.分形几何──数学基础及其应用.沈阳:东北工学院出版社,1991:13017杨国伟.科学通报,1992;37:953` |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|