| 位错密度对大块Fe-3%Si单晶延-脆转变温度的影响 |
| 鲍进生;杨成;哈宽富 |
| 吉林大学 |
|
| EFFECT OF DISLOCATION DENSITY ON DUCTILE-BRITTLE TRANSITION TEMPERATURE IN BULK Fe-3%Si SINGLE CRYSTALS |
| BAO Jinsheng; YANG Cheng; HA Kuanfu(Jilin University; Changchun 130023) |
引用本文:
鲍进生;杨成;哈宽富. 位错密度对大块Fe-3%Si单晶延-脆转变温度的影响[J]. 金属学报, 1995, 31(5): 197-200.
,
,
.
EFFECT OF DISLOCATION DENSITY ON DUCTILE-BRITTLE TRANSITION TEMPERATURE IN BULK Fe-3%Si SINGLE CRYSTALS[J]. Acta Metall Sin, 1995, 31(5): 197-200.