| 含挥发组分B_2O_3渣系活度的测定方法 |
| 戴长虹;张显鹏 |
| 东北大学 |
|
| A METHOD FOR MEASURING ACTIVITIES IN SLAG CONTAINING VOLATILE COMPONENT B_2O_3 |
| DAI Changhong; ZHANG Hianpeng(Northeastern University; Shenyang) |
引用本文:
戴长虹;张显鹏. 含挥发组分B_2O_3渣系活度的测定方法[J]. 金属学报, 1994, 30(18): 243-246.
,
.
A METHOD FOR MEASURING ACTIVITIES IN SLAG CONTAINING VOLATILE COMPONENT B_2O_3[J]. Acta Metall Sin, 1994, 30(18): 243-246.
| 1张子青,周继程,田彦文,吕向明,张晔,丁涌海.全国第五届冶金过程物理化学年会论文集,1984:2542张成涛,MgO-B2O3,SiO2B2O3及MgO-SiO2-B2O3体系的热力学研究,东北大学硕士论文,19883邹元赵彭年,曹兆民.金属学报,1963;6:1214RichardsonFD.PhysicalChemistryofMellsinMetallurgy,NewYork:Academic,1974:1375InghramMG,PorterRF,ChupkaWA.JChemPhys,1956;25:4986RaoBKDP,GaskellDR.MetallTrans,1981;12B:469 |
|