| Si-Mn-Mo系贝氏体钢的CCT图 |
| 刘晓;张明星;陈大明;周鹿宾;康沫狂 |
| 西北工业大学401教研室;西安710072;西北工业大学;西北工业大学;西北工业大学;西北工业大学 |
|
| CCT-DIAGRAM OF Si-Mn-Mo ALLOY SYSTEM BAINITIC STEELS |
| LIU Xiao;ZHANG Mingxing;CHEN Daming;ZHOU Lubin;KANG Mokuang Northwestern Polytechnical University; Xi'an Faculty No.401; Northwestern Polytechnical University; Xi'an 710072 |
引用本文:
刘晓;张明星;陈大明;周鹿宾;康沫狂. Si-Mn-Mo系贝氏体钢的CCT图[J]. 金属学报, 1993, 29(3): 1-5.
,
,
,
,
.
CCT-DIAGRAM OF Si-Mn-Mo ALLOY SYSTEM BAINITIC STEELS[J]. Acta Metall Sin, 1993, 29(3): 1-5.
1 刘晓等,钢铁,待发表 2 康沫狂等,材料科学进展,1988. 2(3) :12 3 Kang M K, Chen D M, Yang D P, Hu G L. Metall Trans. 1992: 23A: 785 4 Cias W W, Doane D V. Metall Trans, 1973; 4A: 225 |
|