| 8090Al-Li合金的疲劳裂纹扩展 |
| 王中光;张匀;胡壮麒;何世禹;李清健 |
| 中国科学院金属研究所;材料疲劳与断裂国家重点实验室;研究员;沈阳(110015)中国科学院金属研究所;中国科学院金属研究所;材料疲劳与断裂国家重点实验室;中国科学院金属研究所;材料疲劳与断裂国家重点实验室;哈尔滨工业大学;哈尔滨工业大学 |
|
| FATIGUE CRACK PROPAGATION IN Al-Li ALLOY 8090 |
| WANG Zhongguang;ZHANG Yun;HU Zhuangqi;HE Shiyu;LI Qingjian State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Academia Sinica; Shenyang Harbin Institute of Technology; Correspendent profersor; Insitute of Research; Acodemia Sinica; Sheyang 110015 |
引用本文:
王中光;张匀;胡壮麒;何世禹;李清健. 8090Al-Li合金的疲劳裂纹扩展[J]. 金属学报, 1992, 28(5): 44-50.
,
,
,
,
.
FATIGUE CRACK PROPAGATION IN Al-Li ALLOY 8090[J]. Acta Metall Sin, 1992, 28(5): 44-50.
1 Jata K V, Starke E A Jr., Metall. Trans., 1986; 17A: 1011 2 Venkateswara Rao K T, Yu W, Ritchie R O. Metall Trans, 1988; 19A: 549 3 Venkateswara Rao K T, Yu W, Ritchie R O. Metall Trans, l988; 19A: 563 4 陈铮.航空学报,1990;11(8) :B369 5 Nicholls D J, Martin J W. Fatigue Fract Eng Mater Struct, 1990; 13: 83 6 Haddleton F L, Murphy S, Griffin T J. J Phys Colloq, 1987; 48 (9) : 809 7 Peters M, Bachmann V, Welpmann K. J Phys Colloq, 1987; 48 (9) : 785 8 HE S Y, Li QJ, Feng X Z, Wang Z G, Zhang Y. Chin J Met Sci Technol, to be published
9 Allen R J, Booth G S, Jutla T. Fatigue Fract Eng Mater Struct, 1988; 11: 45 10 李清健.哈尔滨工业大学硕士学位论文,1991 11 Ritchie R O, Yu W. In: Ritchie R O, Landford J eds., Small Fatigue Cracks, AIME, 1986: 167--189 12 Guiu F, Stevens R N. Fatigue Fract Eng Mater Struct, 1990; 13: 625 13 Miller K J. Fatigue Fract Eng Mater Struct, 1987; 10: 75- |
|