| 在45钢上等离子喷焊Co-Cr结合层的组织结构 |
| 陈汉存;刘正义;庄育智;沈式希 |
| 华南理工大学;华南理工大学机械二系;教授;广州(510641);华南理工大学;华南理工大学 |
|
| STRUCTURE OF BONDING LAYER OF PLASMA SPRAY WELDING OF Co-Cr ALLOY ON PLAIN STEEL |
| CHEN Hancun;LIU Zhengyi;ZHUANG Yuzhi SHEN Shixi South China University of Technology; Guangzhou |
引用本文:
陈汉存;刘正义;庄育智;沈式希. 在45钢上等离子喷焊Co-Cr结合层的组织结构[J]. 金属学报, 1991, 27(2): 37-42.
,
,
,
.
STRUCTURE OF BONDING LAYER OF PLASMA SPRAY WELDING OF Co-Cr ALLOY ON PLAIN STEEL[J]. Acta Metall Sin, 1991, 27(2): 37-42.
1 Savage W F, Nippes E F, Miller T W. Weld J (New York), 1976; 55: 181-s 2 Tong Shushan, Ding Zhangxiong. Advances in Thermal Spraying. Preprint. Proceeding of the 11th International Thermal Spraying Conference, Montreal, Canada, 1986: 691x |
|