| 硼在体心立方结构Fe_3(SiAl)中的分布及其对脆性的改善 |
| 邵元智;顾守仁;陈南平 |
| 清华大学;清华大学材料科学与工程系;副教授北京(100084);清华大学 |
|
| BORON DISTRIBUTION IN BCCINTERMETALLIC COMPOUND Fe_3(Si,Al) AND IMPROVEMENT ON ITS BRITTLENESS |
| SHAO Yuanzhi;GU Shouren;CHEN Nanping Tsinghua University; Beijing |
引用本文:
邵元智;顾守仁;陈南平. 硼在体心立方结构Fe_3(SiAl)中的分布及其对脆性的改善[J]. 金属学报, 1991, 27(2): 27-32.
,
,
.
BORON DISTRIBUTION IN BCCINTERMETALLIC COMPOUND Fe_3(Si,Al) AND IMPROVEMENT ON ITS BRITTLENESS[J]. Acta Metall Sin, 1991, 27(2): 27-32.
1 Liu C T, White C L, Horton J A. Acta Metall, 1985; 33: 213 2 Stoloff N S. High-Temperature Ordered Intermetallic Alloys, Vol. 39. Pittsburgh, Penneylvania: Materials Reseach Society, 1985: 3 3 邵元智,顾守仁,陈南平,清华大学学报(自然科学版), 1989; 29(5) : 25 4 Shao Yuanzhi, Gu Shouren, Chen Nanping. In: C-MRS International'90 Abstracts, June 18--22, 1990, Beijing, China, 1990: 116 5 Koch C C. High-Temperature Ordered Intermetallic Alloys, Vol. 39, Pittsburgh, Penneylvania: Materials Reseach Society, 1985: 397 6 Marcinkowski MJ, Taylor M F. J Mater Sci, 1975; 10: 406 7 Ehlers S K, Mendiratta M G. J Mater Sci, 1984; 19: 2203 8 Crawford R C, Ray I L F, Cockayne D J H. Philos Mag, 1973; 27: 1 9 Marcinkowski M J. In: Thomas G, Washburn J eds., Electron Microscopy and Strength of Crystals, New York: Interscience, 1963: 333 10 Athanassiadis G, Le Caer G, Feet J, Rirnlinger L. Phys Status Solid, 1977; 40A: 425 11 Mendiratta M G. Lipsitt H A. In: C-MRS International'90 Abstracts, June 18--22, 1990, Beijing, China. 1990: 155 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|