| δ-Ni_3Nb对Inconel718合金低周疲劳断裂行为的影响 |
| 洪班德;伊晓;孟庆昌 |
| 哈尔滨工业大学分析测试中心;教授哈尔滨150006;哈尔滨工业大学;哈尔滨工业大学 |
|
| EFFECT OFδ-Ni_3 Nb ON LOW CYCLE FATIGUE RACTURE OF INCONEL 718 |
| HONG Bande;YI Xiao;MENG Qingchang Harbin Institute of Technology |
引用本文:
洪班德;伊晓;孟庆昌. δ-Ni_3Nb对Inconel718合金低周疲劳断裂行为的影响[J]. 金属学报, 1991, 27(1): 55-60.
,
,
.
EFFECT OFδ-Ni_3 Nb ON LOW CYCLE FATIGUE RACTURE OF INCONEL 718[J]. Acta Metall Sin, 1991, 27(1): 55-60.
1 Oblak J M, Paulonis D F, Duvall D S. Metall Trans, 1974; 5: 143 2 Hall R C. Trans ASME, Ser. D: J Basic Eng. 1967; 89: 511 3 Sundararaman M, Mukhopadhyay P, Banerjee S. Metall Trans, 1988; 19A: 453 4 Doswell W, Koul A K, Thamburaj R, Wallace W. NAE-NRCC Report LTR-ST-1596. National Aeronautical Establishment--National Research Council Canada, 1987 5 Sadanada K,Shahinian P.NRL-MR-3727,Naval Research Laboratory Washington,D.C.1978 6 《高温合金金相图谱》编写组.高温合金金相图谱.北京:冶金工业出版社,1979:100 7 上海交通大学《金属断口分析》编写组.金属断口分析.北京:国防工业出版社,1979 8 Mills W J, James L A. J Eng Mater Technol, 1985; 107: 41 9 James L A. Eng Fract Mech, 1986; 25: 305 10 Krueger D D, Antolovich S D, Van Stone R H. Metall Trans, 1987; 18A: 1431 11 Pedron J P, Pineau A. Mater Sci Eng, 1982; 56: 143 12 Merrick H F. Metall Trans, 1974; 5: 891 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|