| 低碳钢冷脆特性参量——临界缺口(裂缝)尺寸的研究 |
| 李道明;姚枚 |
| 哈尔滨工业大学;433信箱;哈尔滨工业大学 |
|
| CRITICAL NOTCH (CRACK) SIZE AS A CHARACTERISTIC PARAMETER OF CRYOGENIC BRITTLENESS IN LOW CARBON STEEL |
| LI Daoming;YAO Mei Harbin Institute of Technology Manuscript received 7 March; 1987; revised manuscript 5 January; 1988 |
引用本文:
李道明;姚枚. 低碳钢冷脆特性参量——临界缺口(裂缝)尺寸的研究[J]. 金属学报, 1988, 24(6): 432-438.
,
.
CRITICAL NOTCH (CRACK) SIZE AS A CHARACTERISTIC PARAMETER OF CRYOGENIC BRITTLENESS IN LOW CARBON STEEL[J]. Acta Metall Sin, 1988, 24(6): 432-438.
1 涂铭旌,鄢文彬,低合金钢低温脆性断裂研究文集,西安交通大学出版社,1985:1--13 2 Knott J F. Fundamentals of Fracture Mechanics, London: Butterworths, 1973: 177--203 3 Ritchie R O, Knott J F, Rice J R. J Mech Phys Solids, 1973; 21: 395--410 4 Oates G. J Iron Steel Inst, 1969; 207: 353 5 姚枚,何裕宽,李道明.钢铁,1984;19(12) :10--18 6 姚枚,李道明,何裕宽.材料学会第一届年会论文集,中国机械工程学会编,1986:123--129 7 Yao M, He Y K, Li D M, Zhou C Z. Advances in Fracture Research, Pergamon Press, Vol. Ⅱ, 1984; 1423--1430 8 Green A P, Hundy B B. J Mevh Phts Solids, 1956; 4: 128--135 9 黄正,姚枚.金属科学与工艺,1987;6(2) :1--7R |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|