| 采用环状裂纹圆棒试样测定中低强度钢的断裂韧度 |
| 刘再华;赵东立 |
| 武汉市喻家山华中工学院力学系;国家机械委成套局 |
|
| MEASUREMENT OF K_(IC) OF MEDIAN OR LOW STRENGTH STEEL USING ROUND BARS WITH CIRCUMFERENCIAL CRACK |
| LIU Zaihua;ZHAO Dongli Huazhong University of Science and Technology; Wuhan Bureau of Complete Sets of Equipment; State Machinery Commission; Beijing Manuscript received 26 January; 1984; revised manuscript 22 August; 1987 |
引用本文:
刘再华;赵东立. 采用环状裂纹圆棒试样测定中低强度钢的断裂韧度[J]. 金属学报, 1988, 24(6): 426-431.
,
.
MEASUREMENT OF K_(IC) OF MEDIAN OR LOW STRENGTH STEEL USING ROUND BARS WITH CIRCUMFERENCIAL CRACK[J]. Acta Metall Sin, 1988, 24(6): 426-431.
1 Jones M H, Bubsey R T, Bucci R J, Collis S F, et al. Development in Fracture Mechanics Test Methods Standardization, ASTM STP 632, 1977: 115--152 2 Bueckner H F. Fracture Toughness and its Applecations, ASTM STP 381, 1965: 82 3 Rice J R, Paris P C, Merkle J G. Progress in Filaw Growth and Fracture Toughness Testing, ASTM STP536, Philadelphia: ASTM, 1973: 231--244 4 肖纪美.金属的韧性与韧化,第二章,上海科技出版社,1980:27--85 5 Hoffman O,Sachs G.乔端,孙梁译.工程塑性力学基础,中国工业出版社,1965:154--157 6 Качанов Л М.周承倜,唐照千译.塑性理论基础,高等教育出版社,1965:203\ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|