| 超塑变形中的晶粒形状效应 |
| 崔建忠;马龙翔 |
| 沈阳东北工学院压力加工系;东北工学院 |
|
| GRAIN SHAPE EFFECT IN SUPERPLASTIC DEFORMATION |
| CUI Jianzhong;MA Longxiang Northeast University of Technology; ShenyangDepartment of Metals Forming;Northeast University of Technology; Shenyang |
引用本文:
崔建忠;马龙翔. 超塑变形中的晶粒形状效应[J]. 金属学报, 1988, 24(4): 354-361.
,
.
GRAIN SHAPE EFFECT IN SUPERPLASTIC DEFORMATION[J]. Acta Metall Sin, 1988, 24(4): 354-361.
1 Suery M, Baudelet B. In: Paton N E, Hamilton C H eds., Superplastic Forming of Structural Alloys, Met Soc AIME, 1982: 105 2 Schneobels J H, Coble R L, Cannon R M. Acta Metall, 1981; 29: 1285 3 松木贤司,针山典笃,时沢贡.日本金属学会志,1981;45:935 4 Wert J A, Paton N E. Metall Trans, 1981; 12A: 1276 5 崔建忠,吴庆龄,马龙翔.东北工学院学报,1987;8:442 6 Raj R, Ashby M F. Metall Trans, 1971; 12: 1113 7 Padmanabhan K A, Davies G J. Superplasticity, New York: Springer, 1980: 15 |
|