| 稀土元素对2.25Cr-1Mo钢断裂性能的影响 |
| 洪友士;W.R.TYSON;B.FAUCHER |
| 北京中关村中国科学院力学研究所;加拿大CANMET物理冶金实验室;加拿大CANMET物理冶金实验室 |
|
| EFFECT OF RARE EARTH ADDITIONS ON FRACTURE PROPERTIES OF 2.25Cr-1Mo STEELS |
| HONG Youshi;W. R. TYSON;B. FAUCHER Institute of Mechanics; Academia Sinica; Beijing; Physical Metallurgy Research Laboratories; CANMET; Ottawa; Canada |
引用本文:
洪友士;W.R.TYSON;B.FAUCHER. 稀土元素对2.25Cr-1Mo钢断裂性能的影响[J]. 金属学报, 1988, 24(4): 282-287.
,
,
.
EFFECT OF RARE EARTH ADDITIONS ON FRACTURE PROPERTIES OF 2.25Cr-1Mo STEELS[J]. Acta Metall Sin, 1988, 24(4): 282-287.
1 Knight R F, Tyson W R, Sproule G I. Met Technol, 1984; 11: 273-279 2 Graham M J, Sproule G I. Ho P. Metall Trans, 1983; 14A: 2558-2560 3 Faucher B, Tyson W R. In: Wessel E T, Loss F J eds. Elastic-Plastic Fracture Test Methods: User's Experience, ASTM STP 856, 1985: 278-293 4 Underwood E E. Quantitative Stereology, Reading, Mass: Addision-Wesley, 1970: 80-147 5 Rice J R, Johnson M A. In: Kanninen M F, Adler W F, Rosenfield A R eds. Inelastic Behaviour of Solids, New York: McGraw-Hill, 1970: 641-672 6 Bates R C. In: Wells J M, Landes J D eds. Fracture: Interactions of Microstructure, Mechanisms, Mechanics (Conference Proceedings), The Metallurgical Society of AIME, 1984: 117-155 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|