γ-TiAl基合金汽车排气阀吸铸充型过程水模拟 |
熊超, 马颖澈, 陈波, 刘奎, 李依依 |
中国科学院金属研究所, 沈阳 110016 |
|
WATER MODELING OF MOULD FILLING DURING SUCTION CASTING PROCESS OF AUTOMOTIVE EXHAUST VALVES OF γ-TiAl BASED ALLOYS |
XIONG Chao, MA Yingche, CHEN Bo, LIU Kui, LI Yiyi |
Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
熊超 马颖澈 陈波 刘奎 李依依. γ-TiAl基合金汽车排气阀吸铸充型过程水模拟[J]. 金属学报, 2011, 47(11): 1408-1417.
,
,
,
,
.
WATER MODELING OF MOULD FILLING DURING SUCTION CASTING PROCESS OF AUTOMOTIVE EXHAUST VALVES OF γ-TiAl BASED ALLOYS[J]. Acta Metall Sin, 2011, 47(11): 1408-1417.
[1] Clemens H, Kestler H. Adv Eng Mater, 2000; 2: 551[2] Yamaguchi M, Inui H, Ito K. Acta Mater, 2000; 48: 307[3] HartfieldWunsch S E, Sperling A A, Morrison R S, DowlingWE, Allison J E. In: Kim YW,Wagner R, Yamaguchi M eds., Gamma Titanium Aluminides. Warrendale, PA: Minerals, Metals and Materials Soc, 1995: 41[4] Dowling W E, Donlon W T, Allison J E. In: Horton J, Baker I, Hanada S, Noebe R D, Schwartz D S eds., High–Temperature Ordered Intermetallic Alloys. Pittsburgh, PA: Materials Research Soc, 1995: 757[5] Gebauer K. Intermetallics, 2006; 14: 355[6] SmarslyW, Baur H, Glitz G, Clemens H, Khan T, Thomas M. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, WhittenbergerJ D eds., Structural Intermetallics 2001, Warrendale, PA: Minerals, Metals and Materials Soc, 2001: 25[7] Chandley G D. AFS Trans, 1976; 84: 37[8] Chandley G D, Cargill D L. AFS Trans, 1990; 98: 413[9] Giese S R, Dix L. AFS Trans, 1999; 107: 217[10] Koitzsch R, Odenthal H J, Pfeifer H. Steel Res Int, 2007; 78: 473[11] Buchholz A, Ji M S, Schmitz W, Engler S. In: Huglen R ed., Technical Session on Light Metals 1997, the 126th TMS Annual Meeting, Worrendale, PA: Minerals, Metals and Materials Soc, 1997: 1043[12] Odenthal H J, Bolling R, Pfeifer H. Steel Res Int, 2003; 74: 35[13] Zhao Z W, Gao Y, Zhang H. Spec cast Nonferrous Alloy, 2007; 27: 351(赵志维, 高永, 张 虎. 特种铸造及有色合金, 2007; 27: 351)[14] Li C Y, Wu S P, Guo J J, Su Y Q, Bi W S, Fu H Z. J Mater Process Technol, 2006; 176: 268[15] Tu X. Basic Theories and Method of Model Experiment. Xi’an: Northwestern Polytechnical University Press, 1989: 51(屠 兴. 模型实验的基本理论与方法. 西安: 西北工业大学出版社, 1989: 51)[16] Bai Y F. PhD Thesis, Harbin Institute of Technology, 2002(白云锋. 哈尔滨工业大学博士论文, 2002)[17] Xia T C. Engineering Fluid Mechanics. Shanghai: Shanghai Jiao Tong University Press, 2006: 5(夏泰淳. 工程流体力学. 上海: 上海交通大学出版社, 2006: 5)[18] Dong X Q, Wang D, Wang C Z, Li Y H, Guo G S, Wang Y C, Liu Z M. Theory and Practice of Low Pressure and Counter Pressure Casting, 3rd Ed., Beijing: China Machine Press, 2003:124(董秀琦, 王冬, 王承志, 李玉海, 郭广思, 王永臣, 刘志明. 低压及差压铸造理论与实践, 第三版. 北京: 机械工业出版社, 2003: 124)[19] Zhou G Q, Yan Z Y, Xu S X, Zhang K B. Fluid Mechanics. Beijing: Higher Education Press, 1992: 88(周光坰, 严宗毅, 许世雄, 章克本. 流体力学. 北京: 高等教育出版社, 1992: 88)[20] He L Q. Engineering Fluid Mechanics. Beijing: China University of Petroleum Press, 2001: 8(贺礼清. 工程流体力学. 北京: 石油大学出版社, 2001: 8) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|