再制造的热喷涂合金涂层的结构完整性与服役寿命预测研究 |
徐滨士, 王海斗, 朴钟宇, 张显程 |
装甲兵工程学院装备再制造技术国防科技重点实验室, 北京 100072 |
|
INVESTIGATION OF STRUCTURAL INTEGRITY AND LIFE TIME PREDICTION OF THE THERMAL SPRAYED ALLOY COATING FOR REMANUFACTURING |
XU Binshi, WANG Haidou, PIAO Zhongyu, ZHANG Xiancheng |
National Key Laboratory for Remanufacturing, Academy of Armored Forces Engineering, Bejing 100072 |
引用本文:
徐滨士 王海斗 朴钟宇 张显程. 再制造的热喷涂合金涂层的结构完整性与服役寿命预测研究[J]. 金属学报, 2011, 47(11): 1355-1361.
,
,
,
.
INVESTIGATION OF STRUCTURAL INTEGRITY AND LIFE TIME PREDICTION OF THE THERMAL SPRAYED ALLOY COATING FOR REMANUFACTURING[J]. Acta Metall Sin, 2011, 47(11): 1355-1361.
[1] Xu B S. China Surf Eng, 2010; 23: 1
(徐滨士. 中国表面工程, 2010; 23: 1)
[2] Xu B S. Remanufacturing Engineering and Its Application. Harbin: Harbin Institute of Technology Press, 2005: 1
(徐滨士. 再制造工程基础及其应用. 哈尔滨: 哈尔滨工业大学出版社, 2005: 1)
[3] Xu B S, Zhu S H. Surface Engineering Theory and Technology. 2nd Ed. Beijing: National Defense Industry Press, 2010: 1
(徐滨士, 朱绍华. 表面工程的理论与技术. 第2版. 北京: 国防工业出版社, 2010: 1)
[4] Zhu Z X, Liu Y, Xu B S, Ma S N. Trans China Weld Inst, 2005; 26: 1
(朱子新, 刘燕, 徐滨士, 马世宁. 焊接学报, 2005; 26: 1)
[5] Wu Z J. Thermal Spray Technology and Applications. Beijing: China Machine Press, 2005: 1
(吴子健. 热喷涂技术与应用. 北京: 机械工业出版社, 2005: 1)
[6] Piao Z Y, Xu B S, Wang H D, Pu C H. Tribol Int, 2010; 43: 252
[7] Zhang X C. PhD Thesis, Shanghai Jiao Tong University, 2007
(张显程. 上海交通大学博士学位论文, 2007)
[8] Zhang X C, Xu B S, Xuan F Z, Wang H D, Wu Y X, Tu S D. J Alloys Compd, 2009; 467: 501
[9] Zhang X C, Xu B S, Wu Y X, Xuan F Z, Tu S D. Appl Surf Sci, 2008; 254: 3879
[10] Zhang X C, Xu B S, Tu S D, Xuan F Z, Wang H D, Wu
Y X. Appl Surf Sci, 2008; 254: 6318 [11] Pfender E. Surf Coat Technol, 1987; 34: 1
[12] Bianchi L, Leger A C, Vardelle M, Vardelle A, Fauchais P. Thin Solid Films, 1997; 305: 35
[13] Gawne D T, Liu B, Bao Y, Zhang T. Surf Coat Technol, 2005; 191: 242
[14] Sampath S, Jiang X, Kulkarni A, Matejicek J, Gilmore D L, Neiser R A. Mater Sci Eng, 2003; A348: 54
[15] Gnaeupel–Herold T, Prask H J, Barker J, Biancaniello F S, Jiggetts R D, Materjicek J. Mater Sci Eng, 2006; A421: 77
[16] Chwa S O, Klein D, Toma F L, Bertrand G, Liao H L, Coddet C, Ohmori A. Surf Coat Technol, 2005; 194: 215
[17] Zhang X C, Xu B S, Xuan F Z, Wang H D, Wu Y S, Tu S D. Wear, 2008; 265: 1875
[18] Zhang X C, Xu B S, Xuan F Z, Tu S D, Wang H D, Wu Y X. Appl Surf Sci, 2008; 254: 3734
[19] Zhang X C, Xu B S, Xuan F Z, Tu S D, Wang H D, Wu Y X. Int J Fatigue, 2009; 31: 906
[20] Holmberg K, Matthews A, Ronkainen H. Tribol Int, 1998; 31: 107 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|