| MORPHOLOGY AND DISTRIBUTION OF Nb-RICH PHASES IN CHILLED CAST IRON |
| FU Li(Shenyang High School of Industry; Shenyang 110044); ZHAI Qijie (University of Science and Technology Beijing; Beijing 100083); ZHENG Guanghua (Anshan Iron and Steel Company; Anshan 114021)(Manuscript received 1995-05-09) |
|
Cite this article:
FU Li(Shenyang High School of Industry; Shenyang 110044); ZHAI Qijie (University of Science and Technology Beijing; Beijing 100083); ZHENG Guanghua (Anshan Iron and Steel Company; Anshan 114021)(Manuscript received 1995-05-09). MORPHOLOGY AND DISTRIBUTION OF Nb-RICH PHASES IN CHILLED CAST IRON. Acta Metall Sin, 1996, 32(2): 159-162.
|
|
|
Abstract The morphology and distribution of Nb-rich phases in chilled cast iron were studied by using STEM. The results demonstrate that there are three morphologies of Nb-rich phases in chilled cast iron, which are lumpy NbC, complicated strip-like phase, and compound with pearlite structure.(Correspondent: FU Li, professor, Foundry Division, Shenyang High School of Industry, Shenyang 110044)
|
|
Received: 18 February 1996
|
| 1陈家祥,炼钢常用图表数据手册.北京:冶金工业出版社,1984:5712陈家祥.炼钢常用图表数据手册.北京:冶金工业出版社,1984;511 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|