| INTERFACES IN PHASE TRANSFORMATIONS |
| J.W.Christian FRS(Department of Materials; Oxford University; Parks Road; Oxford OX1 3PH; UK) |
|
Cite this article:
J.W.Christian FRS(Department of Materials; Oxford University; Parks Road; Oxford OX1 3PH; UK). INTERFACES IN PHASE TRANSFORMATIONS. Acta Metall Sin, 1997, 33(2): 150-156.
|
|
|
Abstract The classification of interfaces in various kinds of phase transformation is discussed.Reconstructive phase transformations have incoherent interfaces and there is no systematic change of shape of the product region. Displacive phase transformations have fully coherent or partly coherent interfaces and are detectable by the change of shape.Fully coherent interfaces include martensitic types in which there is no change of composition and diffusional displacive interfaces in which a change of composition occurs.Both types of interface migrate by the motion of steps or ledges which are also called transformation dislocations in the martensite case. Partly coherent interfaces are also martensitic or diffusional. although examples of the latter type are rare.
|
|
Received: 18 February 1997
|
1 D. Hull, Bull. Inst. Met. 2 (1954) 134. 2 B.A.Bilby and J.W.Christian, The Mechamsm of Phase Transformations in Metals (The Institute of Metals, London, 1956) p. 121. 3 C.Laird and H.I.Aaronson, Acta Metall. 18 (1967) 134. 4 Y.C.Liu and H.I.Aaronson, Acta Metall. 18 (1970) 845. 5 J.M.Howe, H.I.Artonson and R.Gronsky, Acta Metall. 33 (1985) 639. 6 J.W.Christian, Proc. Roy. Soc. London A206 (1951) 51. 7 P. Gaunt and J.W.Christian, Acta Metall. 7 (1959) 529,534. 8 S.Takeuchi and T.Honma, Sci. Rep. Res. Inst. Tohoku Univ. A9 (1957) 492,509. 9 T.Waitz and H.P.Karnthaler, Private communication. 10 C.Hitzenberger and H.P.Karnthaler, Philos. Mag. A64 (1991) 151. 11 T.Waitz and H.P.Karnthaler, Philos. Mag. 1996 in course of publication. 12 H.I.Aaronson and M.G.Hall, Metall. Mater. Trans. 25A (1994) 1797. 13 J.W.Christian, Metall. Mater. Trans. 25A (1994) 1821. 14 R.D.J.Garwood, Inst. Met. 83 (1954) 64. 15 K.Marukawa, 1992: ICOMAT-92, p.821. 16 P.Doig and P.E.J.Flewitt, Met. Sci. l7 (1983) 601. 17 Y.Hamada, M.H.Wu and C.M.Wayman, l992: ICOMAT-92, p.833. 18 Q.H.Li, D.L.Liu and T.Ko, 1992: ICOMAT-92, p.845. 19 T.Ko and S.A.Cottrell, J.Iron Steel Inst. 172 (1952) 307.20 S.A.Cottrell and T.Ko, J.Iron Steel Inst. 173 (1953) 224. 21 H.K.D.H. Bhadeshia, Bainite in Steels (The Institute of Metals, London, 1995). 22 E.Swallow and H.K.D.H.Bhadeshia, In course of publication. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|