CRYSTAL STRUCTURE AND MAGNETIC PROPERTIES OF Y_2Fe_(17-x)Mn_x
YIN Xiaoying;WANG Yingang;TANG Ning;YANG Fuming(State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Chinese People's Public Security University; Beijing 100038)
Cite this article: 

YIN Xiaoying;WANG Yingang;TANG Ning;YANG Fuming(State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Chinese People's Public Security University; Beijing 100038). CRYSTAL STRUCTURE AND MAGNETIC PROPERTIES OF Y_2Fe_(17-x)Mn_x. Acta Metall Sin, 1997, 33(5): 539-542.

Download:  PDF(299KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  X-ray diffraction has proved that the structure of Y2Fe17-xMnx(x≤6.0) compounds is same as Y2Fe17. The study on the lattice constants, Curie temperature and magnetization of the Y2Fe17-xMnx compounds has shown that the lattice constants do not increase continuously with increasing Mn content and have a minimum at x=2.0. The Curie temperature increases from 328 K (x=0.0) to 342 K (x=0.3), and then decreases with increasing Mn content. The saturation magnetization decreases with increasing Mn content.
Key words:  Y_2Fe_(17-x)Mn_x      X-ray diffraction      Curie temperature      magnetization     
Received:  18 May 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I5/539

1 Chafik El Idrissi B,Venturini G,Malaman B Fruchart D.J Less-Common Met, 1991;175:143
2 Jacobs J H,Buschow K H J,Zhou Z F,Liu J P,Li X,De Boer F R.J Magn Magn Mater,1992;104:1275
3 de Boer F R,Zhong X P,Buschow K H J,Jacobs T H,J Magn Magn Mater,1990;90-91:25
4 Franse J J M,Radwanski R J.Handbook of Magnetic Material.Vol.7,Amsterdam:ElsevierScience,1993:384
5 Li Hongshuo,Coey J M D.Handbook of Magnetic Material.Vol.6,Amsterdam:Elsevier Science,1991:73
[1] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[2] LI Yizhuang,HUANG Mingxin. A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction[J]. 金属学报, 2020, 56(4): 487-493.
[3] LI Changji,ZOU Minjie,ZHANG Lei,WANG Yuanming,WANG Sucheng. High-Resolution X-Ray Diffraction Analysis of Epitaxial Films[J]. 金属学报, 2020, 56(1): 99-111.
[4] Weifeng HE, Xiang LI, Xiangfan NIE, Yinghong LI, Sihai LUO. Study on Stability of Residual Stress Induced by Laser Shock Processing in Titanium Alloy Thin-Components[J]. 金属学报, 2018, 54(3): 411-418.
[5] Yutuo ZHANG,Cong LI,Pei WANG,Dianzhong LI. IN SITU SYNCHROTRON X-RAY DIFFRACTION INVESTIGATION ON TENSILE PROPERTIES OF 9Ni STEEL[J]. 金属学报, 2016, 52(4): 403-409.
[6] Shenghua ZHANG,Pei WANG,Dianzhong LI,Yiyi LI. INVESTIGATION OF TRIP EFFECT IN ZG06Cr13Ni4Mo MARTENSITIC STAINLESS STEEL BY IN SITU SYNCHROTRON HIGH ENERGY X-RAY DIFFRACTION[J]. 金属学报, 2015, 51(11): 1306-1314.
[7] WANG Dongmei SONG Lin WANG Yaohui ZHANG Wei Bilige Tegus O. MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS[J]. 金属学报, 2011, 47(3): 344-348.
[8] ZHANG Changsheng MA Tianyu YAN Mi PEI Yongmao GAO Xu. MAGNETOMECHANICAL DAMPING CAPACITY OF <110> ORIENTED Tb0.36Dy0.64(Fe0.85Co0.15)2 ALLOY[J]. 金属学报, 2009, 45(6): 749-753.
[9] Zhao Ning. THE LIQUID STRUCTURE OF SN-CU LEAD-FREE SOLDERS[J]. 金属学报, 2008, 44(4): 467-472 .
[10] Xiang Zhao; Shoujing WANG; GONG Ming-Long; liang zuo. Influence of austenization temperature on the morphology of pearlite in Fe-0.12%C alloy under high magnetic field[J]. 金属学报, 2008, 44(11): 1305-1309 .
[11] Gao-Feng WANG; Lin SONG. Magnetocaloric effect on low field in non-stoichiometric MnFe(P,Si,Ge) alloys[J]. 金属学报, 2007, 43(8): 889-892 .
[12] . [J]. 金属学报, 2007, 43(6): 599-602 .
[13] . Preparation and characterization of Co0.2Zn0.2Mn0.6Fe2O4 nanoparticles by a polymer-pyrolysis route[J]. 金属学报, 2006, 42(5): 497-499 .
[14] LI Xi; REN Zhongming; YU Jianbo; WANG Hui; DENG Kang. Solidification Structure of Primary MnBi Phase in Bi-Mn Alloy Under High Magnetic Field[J]. 金属学报, 2005, 41(7): 685-690 .
[15] JIANG Chuanhai; WU Jiansheng; WANG Dezun. X--Ray Diffraction Analysis for the Recrystallization Behavior Of SiCw/Al Composite at High Temperature[J]. 金属学报, 2004, 40(10): 1023-1026 .
No Suggested Reading articles found!