Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (2): 205-210    DOI:
Current Issue | Archive | Adv Search |
THE PREPARATION OF NbC_x WHISKER
XU Gaiying;LI Jianbao;XIE Zhipeng;HUANG Yong (State Key Laboratory of New Ceramics and Fine Processing; Tsinghua University; Beijing 100084)
Cite this article: 

XU Gaiying;LI Jianbao;XIE Zhipeng;HUANG Yong (State Key Laboratory of New Ceramics and Fine Processing; Tsinghua University; Beijing 100084). THE PREPARATION OF NbC_x WHISKER. Acta Metall Sin, 1998, 34(2): 205-210.

Download:  PDF(1997KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By carbothermal method, the NbCx(x=0.95) whiskers were prepared in graphite resistance furnace under 0.1 MPa/N2 ambient atmosphere at the temperature range of 1120 1670℃. The diameters and lengthes were 50 -1700 urn and 5 -312.5μm respectively. The effect of preparation processing on the apparent morphology and growing machanism of whisker was presented.
Key words:  carbothermal method      NbC_x whisker      processing condition      morphology     
Received:  18 February 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I2/205

1Yu B B, Davis R F.J Phys Chem Solids, 1981; 42: 83
2 Kumashiro Y, Nagai Y, Kat H.J Mater, Sci 1980; 15: 1321
3 Otani S, Tanaka T, Ishizava Y.J Cryst Growth 1983; 62: 211
4 Ohehima K, Harada J. Mater Sci Eng, 1988; A105/106: 29
5Dal B F,Harding S G,Hay D G,Turney T W.J Mater ,Sci,1993;29:6657
6,Sten Anderssonl.Acta Chem Stand, 1965; 19:2285i
[1] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[2] LI Min, LI Haoze, WANG Jijie, MA Yingche, LIU Kui. Effect of Ce on the Microstructure, High-Temperature Tensile Properties, and Fracture Mode of Strip Casting Non-Oriented 6.5%Si Electrical Steel[J]. 金属学报, 2022, 58(5): 637-648.
[3] ZHANG Xinfang, YAN Longge. Regulating the Non-Metallic Inclusions by Pulsed Electric Current in Molten Metal[J]. 金属学报, 2020, 56(3): 257-277.
[4] LIU Haixia, CHEN Jinhao, CHEN Jie, LIU Guanglei. Characteristics of Waterjet Cavitation Erosion of 304 Stainless Steel After Corrosion in NaCl Solution[J]. 金属学报, 2020, 56(10): 1377-1385.
[5] SONG Xuexin, HUANG Songpeng, WANG Chuan, WANG Zhenyao. The Initial Corrosion Behavior of Carbon Steel Exposed to the Coastal-Industrial Atmosphere in Hongyanhe[J]. 金属学报, 2020, 56(10): 1355-1365.
[6] Chengming ZHENG, Qingchao TIAN. Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel[J]. 金属学报, 2019, 55(4): 427-435.
[7] Wensheng XU, Wenzheng ZHANG. An Investigation of the Crystallography of Pearlites Nucleated on the Proeutectoid Cementite[J]. 金属学报, 2019, 55(4): 496-510.
[8] JIN Chenri, YANG Suyuan, DENG Xueyuan, WANG Yangwei, CHENG Xingwang. Effect of Nano-Crystallization on Dynamic Compressive Property of Zr-Based Amorphous Alloy[J]. 金属学报, 2019, 55(12): 1561-1568.
[9] YANG Gaolin, LIN Xin, LU Xiangang. Crystallization Morphology and Evolution Mechanism of Laser Multiple Remelting of Zr55Cu30Al10Ni5 Metallic Glass[J]. 金属学报, 2019, 55(12): 1544-1550.
[10] CAO Lihua, CHEN Yinbo, SHI Qiyuan, YUAN Jie, LIU Zhiquan. Effects of Alloy Elements on the Interfacial Microstructure and Shear Strength of Sn-Ag-Cu Solder[J]. 金属学报, 2019, 55(12): 1606-1614.
[11] Baogang WANG, Hongliang YI, Guodong WANG, Zhichao LUO, Mingxin HUANG. Reconstruction of 3D Morphology of TiB2 in In Situ Fe Matrix Composites[J]. 金属学报, 2019, 55(1): 133-140.
[12] Siqian BAO, Bingbing LIU, Gang ZHAO, Yang XU, Shanshan KE, Xiao HU, Lei LIU. Three-Dimensional Morphologies of Abnormally Grown Goss Oriented Grains in Hi-B Steel During Secondary Recrystallization Annealing[J]. 金属学报, 2018, 54(6): 877-885.
[13] Huijun KANG, Jinling LI, Tongmin WANG, Jingjie GUO. Growth Behavior of Primary Intermetallic Phases and Mechanical Properties for Directionally Solidified Al-Mn-Be Alloy[J]. 金属学报, 2018, 54(5): 809-823.
[14] Min LI, Jing LIU, Qingwei JIANG. Effect of Annealing Temperature on Tensile Fracture Behavior of ARB-Cu at Room Temperature[J]. 金属学报, 2017, 53(8): 1001-1010.
[15] Jing GUO,Hanjie GUO,Keming FANG,Shengchao DUAN,Xiao SHI,Wensheng YANG. Morphology Prediction Theory and Experimental Measurement for the Secondary Phase Particle in Steel[J]. 金属学报, 2017, 53(7): 789-796.
No Suggested Reading articles found!