| THE PREPARATION OF NbC_x WHISKER |
| XU Gaiying;LI Jianbao;XIE Zhipeng;HUANG Yong (State Key Laboratory of New Ceramics and Fine Processing; Tsinghua University; Beijing 100084) |
|
Cite this article:
XU Gaiying;LI Jianbao;XIE Zhipeng;HUANG Yong (State Key Laboratory of New Ceramics and Fine Processing; Tsinghua University; Beijing 100084). THE PREPARATION OF NbC_x WHISKER. Acta Metall Sin, 1998, 34(2): 205-210.
|
|
|
Abstract By carbothermal method, the NbCx(x=0.95) whiskers were prepared in graphite resistance furnace under 0.1 MPa/N2 ambient atmosphere at the temperature range of 1120 1670℃. The diameters and lengthes were 50 -1700 urn and 5 -312.5μm respectively. The effect of preparation processing on the apparent morphology and growing machanism of whisker was presented.
|
|
Received: 18 February 1998
|
1Yu B B, Davis R F.J Phys Chem Solids, 1981; 42: 83 2 Kumashiro Y, Nagai Y, Kat H.J Mater, Sci 1980; 15: 1321 3 Otani S, Tanaka T, Ishizava Y.J Cryst Growth 1983; 62: 211 4 Ohehima K, Harada J. Mater Sci Eng, 1988; A105/106: 29 5Dal B F,Harding S G,Hay D G,Turney T W.J Mater ,Sci,1993;29:6657 6,Sten Anderssonl.Acta Chem Stand, 1965; 19:2285i |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|