HIGH TEMPERATUER LOW CYCLE FATIGUE OF DZ40M COBALT-BASE SUPERALLOY
JIANG Wenhui; YAO Xiangdong; GUAN Hengrong; HU Zhuangqi ( Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Shenyang Polytechnic University; Shenyang 110023)
Cite this article: 

JIANG Wenhui; YAO Xiangdong; GUAN Hengrong; HU Zhuangqi ( Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Shenyang Polytechnic University; Shenyang 110023). HIGH TEMPERATUER LOW CYCLE FATIGUE OF DZ40M COBALT-BASE SUPERALLOY. Acta Metall Sin, 1998, 34(4): 378-383.

Download:  PDF(2754KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Stress controlled low cycle fatigue tests on directionally solidified cobalt-basesuperalloy DZ40M have been conducted at 900℃ in ambient atmosphere. DZ40M superalloy exhibits high low cycle fatigue resistance. The fractography observation indicates that preferentially oxidized carbides at specimen surface act as crack initiation sites, and carbides in matrix have the retardation effect on crack propagation. Oxdation effect reduces alloy ductility, thatpromotes crack propagation. High temperature low cycle fatigue damage of DZ40M superalloyresults from the interaction of thermo--mechanical fatigue and enviromental okidation.
Key words:  directional solidification      cobalt-base superalloy      low cycle fatigue      high temperature oxidation      fracture analysis     
Received:  18 April 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I4/378

1姚向东,张静华,张志亚,李英敖,赵乃仁,管恒荣.胡壮麒.金属学报,1995;31:A320(Yao Xiangdong, Zhang Jinghua, Zhang Zhiya, Li Ying'ao, Zhao Nairen, Guan hengrong, Hu Zhuangqi.Acta Metall Sin, 1995; 31: A320)
2 刘培生. 中国科学院金属研究所硕士学位论文, 1996(Liu Peisheng. Master Thesis, Institute of Metal Research, The Chinese Academy of Sciences,Shenyang, 1996)
3 Merrick H F. Metall Trans, 1971; 5: 891
4 Antolovich S D, Liu S, Baur R. Metall Trans, 1981; 12A: 473
5 Sims C T. J Met, 1969; 21: 27
6 Reuchet J, Remy L. Mater Sci Eny, 1983; 58: 19
7 Vandermousen R F, Viatour P, Drapier J M, Coutsouradis D. Cobalt, 1974; (1): 6
8 Reuchet J, Remy L. Mater Sci Eng, 1983; 58; 33
9 美国金属学会主编. 邓日红, 朱之琴, 吴世泽等译, 金属手册. 第八版, 第九卷, 北京.: 机械工业出版社, 1983: 197(American Society for Metals ed. Deng Rihong, Zhu Zhiqin, Wu Shize et al trans. Metal Handbook. 8th Edition, Vol.9, Beijing: Mechanical Industry Press, 1983; 197)
[1] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[4] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[5] LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie. Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. 金属学报, 2022, 58(8): 1072-1082.
[6] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[7] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[8] YANG Liang, LV Haotian, WAN Chunlei, GONG Qianming, CHEN Hao, ZHANG Chi, YANG Zhigang. Review: Mechanism of Reactive Element Effect—Oxide Pegging[J]. 金属学报, 2021, 57(2): 182-190.
[9] ZHANG Xiaoli, FENG Li, YANG Yanhong, ZHOU Yizhou, LIU Guiqun. Influence of Secondary Orientation on Competitive Grain Growth of Nickel-Based Superalloys[J]. 金属学报, 2020, 56(7): 969-978.
[10] ZHANG Jian,WANG Li,WANG Dong,XIE Guang,LU Yuzhang,SHEN Jian,LOU Langhong. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2019, 55(9): 1077-1094.
[11] XU Qingyan,YANG Cong,YAN Xuewei,LIU Baicheng. Development of Numerical Simulation in Nickel-Based Superalloy Turbine Blade Directional Solidification[J]. 金属学报, 2019, 55(9): 1175-1184.
[12] Mingyu ZHAO,Huijuan ZHEN,Zhihong DONG,Xiuying YANG,Xiao PENG. Preparation and Performance of a Novel Wear-Resistant and High Temperature Oxidation-Resistant NiCrAlSiC Composite Coating[J]. 金属学报, 2019, 55(7): 902-910.
[13] Hui FANG,Hua XUE,Qianyu TANG,Qingyu ZHANG,Shiyan PAN,Mingfang ZHU. Dendrite Coarsening and Secondary Arm Migration in the Mushy Zone During Directional Solidification:[J]. 金属学报, 2019, 55(5): 664-672.
[14] Yan YANG, Guangyu YANG, Shifeng LUO, Lei XIAO, Wanqi JIE. Microstructures and Growth Orientation of Directionally Solidification Mg-14.61Gd Alloy[J]. 金属学报, 2019, 55(2): 202-212.
[15] JIN Hao, JIA Qing, LIU Ronghua, XIAN Quangang, CUI Yuyou, XU Dongsheng, YANG Rui. Seed Preparation and Orientation Control of PST Crystals of Ti-47Al Alloy[J]. 金属学报, 2019, 55(12): 1519-1526.
No Suggested Reading articles found!