CYCLIC DEFORMATION BEHAVIOR OF [011] MULTIPLE-SLIP-ORIENTED COPPER SINGLE CRYSTALSCyclic Stress-Strain Response
LI Xiaowu; WANG Zhongguang; SUN Shouguang; WU Shiding;LI Shouxin;LI Guangyi (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Department of Mechanical Engineering; Northern Jiaotong University; Beijing 100044)
Cite this article:
LI Xiaowu; WANG Zhongguang; SUN Shouguang; WU Shiding;LI Shouxin;LI Guangyi (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Department of Mechanical Engineering; Northern Jiaotong University; Beijing 100044). CYCLIC DEFORMATION BEHAVIOR OF [011] MULTIPLE-SLIP-ORIENTED COPPER SINGLE CRYSTALSCyclic Stress-Strain Response. Acta Metall Sin, 1998, 34(5): 545-551.
Abstract Cyclic deformation behavior of [011] multiple-slip-oriented copper single crystals was investigated with the plastic resolved shear strain amplitudes (γp1) in the range of 1.1 × 10-4 - 7.2× 10-3. It is shown that the cyclic deformation behavior of [011] copper single crystal is quite different from that of [001] and [111] multiple-slip-oriented crystals. [011] crystals exhibit rather low initial hardening rate, which does not increase notably even under higher plastic strain amplitudes. The cyclic stress-strain curve (CSSC) of [011] crystal shows a plateau region over the range of 1.1 × 10-4 - 7.2 × 10-3. The occurrence of plateau region in CSSC is mainly determined by the slip characteristics and the corresponding dislocation reactions in the crystal. Moreover,the hysteresis loop shape parameter VH could be efficiently employed to determine the nucleation stress of PSBs in [011] multiple-slip-oriented copper single crystal.
1Basinski Z S, Basinski S J Pine Mater Sci, 1992; 36: 89 2Chung Y D, Margolin H. Metall Trans, 1973; 4: 1905 3Lepisto T K, Kettunen P O Mater Sci Eng, 1986 83: 1 4Villechaise P, Mendez J, Violan P. Acta Metall Mater, 1991; 39: 1683 5Jin N Y, Winter A T Acta Metall, 1984; 32: 1173 6Gong B,Wang Z R,Wang Z G.Acta Mater,1997;45:1365 7Wang Z R; Gong B, Wang Z G. Acta Mater, 1997 45: 1379 8Jin N Y.Philos Mag Lett,1987;56:23 9Gong B, Wang Z R, Wang Z G, Zhang Y W. Mater Sci Eng, 1996; A210: 94 10Mughrabi H. Mater Sci Eng, 1978; 33: 207 11宫波,王中光,张轶伟、李广义,张天宜.金属学报,1994; 30:431(Gong Bo,Wang Zhongguang,Zhang Yiwei,Li Guangyi;Zhang Tianyi.Acta Metall Sin,1994; 30:431) 12张轶伟.中国科学院金属研究所硕士学位论文,1995(Zhang Yiwei. Master Dissertation, Institute of Metal Research, The Chinese Acadeny of Sciences, 1995) 13Franciosi P, Berveiller M, Zaoui A. Acta Metall, 1980; 28: 273 14 Franciosi P,Zaoui A Acta Metall ,1982;30:1627 15Cheng A S, Laird C Mater Sci Eng, 1981; 56: 111 16Winter A T. Philos Mag, 1974; 29: 719 17Jin N Y. Acta Metall,1989;37:2055 18Polak J, Helesic J, Obrlik K. Mater Sci Eng, 1988; A101: 7m
ZHANG Zhefeng; WANG Zhongguang; SU Huihe(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: ZHANG Zhefeng Tel: (024)23843531-55225; Fax: (024)23891320. CYCLIC DEFORMATION BEHAVIOR OF A COPPER BICRYSTAL WITH A PERPENDICULAR GRAIN BOUNDARY[J]. 金属学报, 1998, 34(8): 841-846.
I. Cyclic Deformation Behavior and Slip Morphology HU Yunming; WANG Zhongguang (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy ofSciences; Shenyang 110015) (Manuscript received 1996-09- 12; in revised form 1997-03-07). CYCLIC DEFORMATION BEHAVIOR AND FATIGUE CRACK INIT1ATION IN COPPER BICRYSTALS[J]. 金属学报, 1997, 33(8): 814-823.
GU Yuefeng;LIU Yi;LIN Dongliang(T.L.Lin)(Shanghai Jiaotong University;Shanghai 200030);GUO Jianting(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-01-13;in revised form 1995-07-03). CYCLIC DEFORMATION BEHAVIOUR OF Ni_3(Al,Zr) SINGLE CRYSTAL AT ROOM TEMPERATURE[J]. 金属学报, 1995, 31(11): 513-518.