| INTERFACE REACTION BETWEEN CERAMIC MOULDS AND Ti46Al1B AS--CAST VALVES |
| MA Yingche; WANG Weidong; CHEN Bo; GAO Ming; LIU Kui; LI Yiyi |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
MA Yingche WANG Weidong CHEN Bo GAO Ming LIU Kui LI Yiyi. INTERFACE REACTION BETWEEN CERAMIC MOULDS AND Ti46Al1B AS--CAST VALVES. Acta Metall Sin, 2009, 45(3): 369-373.
|
|
|
Abstract Al2O3 and Y2O3 were used as surface materials of shell mould to centrifugal--cast Ti46Al1B (atomic fraction, %) valves, the interface reaction between shell and alloy and its mechanism were analyzed by SEM and XRD, and oxygen increment in the castings was measured by gas analysis. The results show that the reaction layer thicknesses of Y2O3 and Al2O3 shells are about 90 and 170 μm, respectively, indicating Y2O3 shell has better thermodynamic stability and smaller increment of oxygen in casting than Al2O3 shell, which is accordant with thermodynamic calculation. So the Y2O3 mould is fitter for casting Ti46Al1B valves than Al2O3 mould.
|
|
Received: 21 August 2008
|
|
|
| [1] Kim Y W. Mater Sci Eng, 1995; A192–193: 519
[2] Kim Y W. Acta Metall, 1999; 12: 334
[3] LorettoMH, HorspoolD, Botten R, HuD, Li Y G, Srivastava D, Sharman R, Wu X. Mater Sci Eng, 2002; A329–331: 1
[4] Yamaguchi M, Inui H. In: Daloria R, Lewwandowski J J, Liu C T, Martin P L, Miracle D B, Nathal M V, eds., Structural Intermetallics, Warrendale: TMS, 1993: 127
[5] Lapin J, Nazmy M. Mater Sci Eng, 2004; A380: 298
[6] Klaus G. Intermetallics, 2006; 14: 355
[7] Liu K, Ma Y C, Gao M, Rao G B, Li Y Y, Wei K, Wu X H, Loretto M H. Intermetallics, 2005; 13: 925
[8] Blum M, Jarczyk G, Scholz H, Pleier S, Busse P, Laudenberg H J, Segtrop K, Simon R. Mater Sci Eng, 2002; A329–331: 616
[9] Sommer A W, Keijzers G C. In: Kim Y W, Clemens H, Rosenberger A H, eds., Gamma Titanium Aluminides, Warrendale: TMS, 2003: 3
[10] Jia Q, Cui Y Y, Yang R. Acta Metall Sin, 2002; 38: 351
(贾清, 崔玉友, 杨锐. 金属学报, 2002; 38: 351)
[11] Jia Q, Cui Y Y, Yang R. J Mater Sci, 2006; 41: 3045
[12] Jones S, Bentley S A, Marquis P M. Br Ceram Trans, 2002; 101: 100
[13] Nan H, Xie C M. Acta Metall Sin, 2002; 38: 345
(南海, 谢成木. 金属学报, 2002; 38: 345)
[14] Yan C F, Zhao G J, Hang Y, Xu J. J Synth Cryst, 2005; 34: 144
(严成锋, 赵广军, 杭寅, 徐军. 人工晶体学报, 2005; 34: 144)
[15] Kobayashi Y, Tsukihashi F. High Temp Mater Processes, 2000; 19: 211 |