Abstract Abstract: The wetting behavior of Pd60-Ni40,PdNi-(3~6)V,PdNi-(7~15)V and PdNi-(16~24)Cr-(6~15)V on Si3N4 was studied by the sessile drop method. The results show that on the condition heating at 1250℃ for 30 min in vacuum, small contact angle and excellent interface are obtained using PdNi-(16~24)Cr-(6~15)V brazing filler. In the interfacial layer with this brazing filler, elements Cr and V preferentially diffused to Si3N4 and resulted in the reaction products of Cr-N phase and V-N phase. A small amount of element Si reacted with elements Cr and V and formed Cr-Si phase and V-Si phase. The matrix of filler metal was composed of Pd-Ni solid solution with some element Si, Pd-Si phase and Ni-Si phase. When the elements Cr and V were added concurrently in the brazing filler, the former diffused to the reaction layer more strongly than the latter.
[1]Xian A P,Si Z Y.J Mater Sci,1992;27:1560 [2]Naka M,Kubo M.Trans JWRI,1987;16(1):83 [3]Naka M,Kubo M.J Mater Sci,1987;22:4417 [4]Xiong H P,Mao W,Cheng Y Y,Li X H,Guo W L.J Mater Sci Lett,2001;20:1681 [5]Loehman R E.Key Eng Mater,1999;161-163:657 [6]Hadian A M,Robin A L D.J Am Ceram Soc,1996;79: 659 [7]Xiong H P,Mao W,Xie Y H,Chen B,Guo W L,Li X H, Cheng Y Y.J Mater Res,2007;56:173 [8]Okamura H.Weld Int,1993;7:236 [9]Kang S,Kim H J.Weld J,1995;74(9):289 [10]Ceccone G,Nicholas M G,Peteves S D,Kodentsov A A, Kivilahti J K,Van Loo F J J.J Eur Ceram Soc,1995;15: 563 [11]Xiong H P,Cheng Y Y,Mao W,Guo W L,Li X H,Xie Y H,Pan H.Acta Metall Sin,2000;36:1269 (熊华平,程耀永,毛唯,郭万林,李晓红,谢永慧,潘辉.金属学报,2000;36:1269) [12]Gotman I,Gutmanas E Y.Acta Metall Mater,1992;40: 121 [13]Fukai T,Naka M,Schuster J C.Trans JWRI,1997;26(1): 93 [14]Bhanumurthy K,Schmid-Fetzer R.Composites,2001; 32A:569 [15]Xiong H P,Chen B,Kang Y S,Mao W,Kawasaki A,Oka- mura H,Watanabe R.Scr Mater,2007;56:173 [16]Park J S,Landry K,Perepezko J H.Mater Sci Eng,1999; A259:279