Abstract  Abstract: The wetting behavior of Pd60-Ni40,PdNi-(3~6)V,PdNi-(7~15)V and PdNi-(16~24)Cr-(6~15)V on Si3N4 was studied by the sessile drop method. The results show that on the condition heating at 1250℃ for 30 min in vacuum, small contact angle and excellent interface are obtained using PdNi-(16~24)Cr-(6~15)V brazing filler. In the interfacial layer with this brazing filler, elements Cr and V preferentially diffused to Si3N4 and resulted in the reaction products of Cr-N phase and V-N phase. A small amount of element Si reacted with elements Cr and V and formed Cr-Si phase and V-Si phase. The matrix of filler metal was composed of Pd-Ni solid solution with some element Si, Pd-Si phase and Ni-Si phase. When the elements Cr and V were added concurrently in the brazing filler, the former diffused to the reaction layer more strongly than the latter.
Key words:       
Received:  12 September 2007     
ZTFLH:  TG454  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I10/1260

[1]Xian A P,Si Z Y.J Mater Sci,1992;27:1560
[2]Naka M,Kubo M.Trans JWRI,1987;16(1):83
[3]Naka M,Kubo M.J Mater Sci,1987;22:4417
[4]Xiong H P,Mao W,Cheng Y Y,Li X H,Guo W L.J Mater Sci Lett,2001;20:1681
[5]Loehman R E.Key Eng Mater,1999;161-163:657
[6]Hadian A M,Robin A L D.J Am Ceram Soc,1996;79: 659
[7]Xiong H P,Mao W,Xie Y H,Chen B,Guo W L,Li X H, Cheng Y Y.J Mater Res,2007;56:173
[8]Okamura H.Weld Int,1993;7:236
[9]Kang S,Kim H J.Weld J,1995;74(9):289
[10]Ceccone G,Nicholas M G,Peteves S D,Kodentsov A A, Kivilahti J K,Van Loo F J J.J Eur Ceram Soc,1995;15: 563
[11]Xiong H P,Cheng Y Y,Mao W,Guo W L,Li X H,Xie Y H,Pan H.Acta Metall Sin,2000;36:1269 (熊华平,程耀永,毛唯,郭万林,李晓红,谢永慧,潘辉.金属学报,2000;36:1269)
[12]Gotman I,Gutmanas E Y.Acta Metall Mater,1992;40: 121
[13]Fukai T,Naka M,Schuster J C.Trans JWRI,1997;26(1): 93
[14]Bhanumurthy K,Schmid-Fetzer R.Composites,2001; 32A:569
[15]Xiong H P,Chen B,Kang Y S,Mao W,Kawasaki A,Oka- mura H,Watanabe R.Scr Mater,2007;56:173
[16]Park J S,Landry K,Perepezko J H.Mater Sci Eng,1999; A259:279
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!