    					| EFFECT OF ROLLING PROCESS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF 7050 ALUMINUM ALLOY | 
  					 
  					  															
						| 中国科学院金属研究所 | 
					 
										
						 | 
					 
				 
				
				Cite this article: 
				
					
			      . EFFECT OF ROLLING PROCESS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF 7050 ALUMINUM ALLOY. Acta Metall Sin, 2008, 44(1): 49-54        .	
				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
              
				
												  
													
													    | 
													    	
														 | 
													 
																										
													
														| 
															
													     		                            						                            																	    Abstract  The effect of rolling reduction and temperature on the microstructure and mechanical properties of 7050 aluminum alloy was investigated. For the sample with a rolling deformation of 30%, most of dendritic structure remained. When the rolling reduction increased to 70%, the cast structure disappeared with the microstructure being characterized by the subgrains and recrystallized grains. Some coarse phases were identified to be Al7Cu2Fe and Al2CuMg by DSC and EDS. The Al7Cu2Fe with a cluster distribution did not dissolve into the matrix, whereas the globular shape of the Al2CuMg phase suggested partial dissolution during the heat treatment. The fraction of the recrystallized grains in the samples rolled under a reduction of 70 and 90% was 1.25 and 12.4%, respectively. The sample rolled under a rolling reduction of 70% exhibited the highest strength and hardness. The sample rolled at 300oC had a lot of recrystallized grains. At 430oC, improved material flow and the occurrence of dynamic recovery reduced stored deformation energy, thereby decreasing the amount of recrystallized grains. In this case, the sample exhibited the highest strength and hardness.
																										     | 
														 
												  		
														
															| 
															    																	Received:  14 June 2007
																	    
															    															    															  
															 | 
															
														 
														 														
															| 
																
															 | 
														 
																																									    																											 
												 
												
												
												
												 
												
												  
             
                         
            
									            
									               
																												  
															  [1]Wang T,Yin Z M.J Rare Met,2006;30:197 (王涛,尹志民.稀有金属,2006;30:197)  [2]Wagner J A,Shenoy R N.Metall Trans,1991;22A:2809  [3]Dai X Y,Xia C Q,Wu A R,Wang J W,Li Y Y.Mater Rev,2006;20(5):104 (戴晓元,夏长清,吴安如,王杰文,李杨勇.材料导报,2006;20(5):104)  [4]Wang Z T,Tian R Z.Handbook of Aluminum Alloy and Processing.3rd ed.,Changsha:Central South University Press,2005:927 (王祝堂,田荣璋.铝合金及其加工手册.第3版,长沙:中南大学出版社,2005:927)  [5]Tian F Q,Li N K,Cui J Z.Light Alloy Fabr Technol, 2005;33(12):1 (田福泉,李念奎,崔建忠.轻合金加工技术,2005;33(12):1)  [6]Sha G,Cerezo A.Acta Mater,2004;52:4503  [7]Dumont D,Deschamps A,Brechet Y.Mater Sci Eng, 2003;A356:326  [8]Lin J C,Liao H L,Jehng W D,Chang C H,Lee S L. Corros Sci,2006;48:3139  [9]Oliveira A F,Barros M C,Cardoso K R,Travessa D N. Mater Sci Eng,2004;A379:321  [10]Deshpande N U,Gokhale A M,Denzer D K,Liu J.Metall Mater Trans,1998;29A:1191  [11]Fan X G,Jiang D M,Meng Q C,Zhong L.Mater Lett, 2006;60:1475  [12]Robson J D,Prangnell P B.Acta Mater,2001;49:599  [13]Li X M,Starink M J.Mater Sci Technol,2001;17:1324  [14]Starink M J,Wang S C.Acta Mater,2003;51:5131  [15]Robson J D,Prangnell P B.Mater Sci Technol,2002;18: 607 | 
														   
																											 
									             
									           
             
			            			 
			
             
								                
															
																
																	
																																																																									
																				| No Suggested Reading articles found! | 
																			 
																																			 
																 | 
															 
														 
								             
             
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |