Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (1): 49-54     DOI:
Research Articles Current Issue | Archive | Adv Search |
EFFECT OF ROLLING PROCESS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF 7050 ALUMINUM ALLOY
中国科学院金属研究所
Cite this article: 

. EFFECT OF ROLLING PROCESS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF 7050 ALUMINUM ALLOY. Acta Metall Sin, 2008, 44(1): 49-54 .

Download:  PDF(751KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of rolling reduction and temperature on the microstructure and mechanical properties of 7050 aluminum alloy was investigated. For the sample with a rolling deformation of 30%, most of dendritic structure remained. When the rolling reduction increased to 70%, the cast structure disappeared with the microstructure being characterized by the subgrains and recrystallized grains. Some coarse phases were identified to be Al7Cu2Fe and Al2CuMg by DSC and EDS. The Al7Cu2Fe with a cluster distribution did not dissolve into the matrix, whereas the globular shape of the Al2CuMg phase suggested partial dissolution during the heat treatment. The fraction of the recrystallized grains in the samples rolled under a reduction of 70 and 90% was 1.25 and 12.4%, respectively. The sample rolled under a rolling reduction of 70% exhibited the highest strength and hardness. The sample rolled at 300oC had a lot of recrystallized grains. At 430oC, improved material flow and the occurrence of dynamic recovery reduced stored deformation energy, thereby decreasing the amount of recrystallized grains. In this case, the sample exhibited the highest strength and hardness.
Key words:       
Received:  14 June 2007     
ZTFLH:  TG146.2  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I1/49

[1]Wang T,Yin Z M.J Rare Met,2006;30:197 (王涛,尹志民.稀有金属,2006;30:197)
[2]Wagner J A,Shenoy R N.Metall Trans,1991;22A:2809
[3]Dai X Y,Xia C Q,Wu A R,Wang J W,Li Y Y.Mater Rev,2006;20(5):104 (戴晓元,夏长清,吴安如,王杰文,李杨勇.材料导报,2006;20(5):104)
[4]Wang Z T,Tian R Z.Handbook of Aluminum Alloy and Processing.3rd ed.,Changsha:Central South University Press,2005:927 (王祝堂,田荣璋.铝合金及其加工手册.第3版,长沙:中南大学出版社,2005:927)
[5]Tian F Q,Li N K,Cui J Z.Light Alloy Fabr Technol, 2005;33(12):1 (田福泉,李念奎,崔建忠.轻合金加工技术,2005;33(12):1)
[6]Sha G,Cerezo A.Acta Mater,2004;52:4503
[7]Dumont D,Deschamps A,Brechet Y.Mater Sci Eng, 2003;A356:326
[8]Lin J C,Liao H L,Jehng W D,Chang C H,Lee S L. Corros Sci,2006;48:3139
[9]Oliveira A F,Barros M C,Cardoso K R,Travessa D N. Mater Sci Eng,2004;A379:321
[10]Deshpande N U,Gokhale A M,Denzer D K,Liu J.Metall Mater Trans,1998;29A:1191
[11]Fan X G,Jiang D M,Meng Q C,Zhong L.Mater Lett, 2006;60:1475
[12]Robson J D,Prangnell P B.Acta Mater,2001;49:599
[13]Li X M,Starink M J.Mater Sci Technol,2001;17:1324
[14]Starink M J,Wang S C.Acta Mater,2003;51:5131
[15]Robson J D,Prangnell P B.Mater Sci Technol,2002;18: 607
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!