| The numerical simulation of interaction between melting pool and metal powder during laser rapid forming |
| W.P.Jia;;;; |
|
Cite this article:
W.P.Jia. The numerical simulation of interaction between melting pool and metal powder during laser rapid forming. Acta Metall Sin, 2007, 43(5): 546-552 .
|
|
|
Abstract The Laser Rapid Forming (LRF), an advanced solid freedom fabrication technology, has a bright future in manufacturing of high performance dense metal components with complex structure in aero, spaceflight and many other fields. During LRF, the melting pool free surface serves as a moving window of laser power and powder mass input and a dynamic boundary of the LRF continuous growth domain, so the interaction between laser, powder and melting pool free surface is the basic problem that should be coped with in LRF process. In this paper, the melting pool transient temperature field and gas/powder two phase fluid field numerical model are established. Using finite element birth and death technology, the growth of cladding layers and shape of melting pool free surface are simulated, and using Lagrangian particle tracking model and momentum loss (parallel and perpendicular)option, the interaction between melting pool free surface and powder such as capture and reflect are simulated. At last, the interaction between 316L stainless steel powder, laser and melting pool free surface is calculated, and the numerical result is in agreement with that of the experiment.
|
|
Received: 20 September 2006
|
|
|
[1] Mazumder J, Dutta D, Kikuchi N, Ghosh A. Opt Lasers Eng, 2000; 34: 397 [2] Chen J, Tan H, Yang H O, Xiong J T, Huang W D. Appl Laser,2005; 25(2): 77 (陈静,谭华,杨海欧,熊江涛,黄卫东.应用激光,2005; 25(2)77) [3] Fu Y C, Loredo A, Martin B, Vannes A B .J Mater Process Technol, 2002; 128: 106 [4] Liu Z X, Chen J, Huang W D, Wu D Y. Chin J Lasers, 2004; 31: 875 (刘振侠,陈静,黄卫东,吴丁毅.中国激光,2004;31:875) [5] Lin J. Opt Lasers Technol, 1999; 31: 233 [6] Xi M Z, Zhang Y Z, Shi L K, Gao S Y. Chin J Nonferrous Met, 2003; 13: 887 (席明哲,张永忠,石力开,高士友.中国有色金属学报,2003; 13:887) [7] Toyserkani E, Khajepour A, Corbin S. Opt Lasers Eng, 2004; 41: 849 [8] Huang Y L, Zou D N, Liang G Y, Su J Y. flare Met Mater Eng, 2003; 32: 330 (黄延禄,邹德宁,梁工英,苏俊义.稀有金属材料与工程,2003; 32:330) [9] Powell J. PhD Dissertation, Imperial College of Science and Technology, London, 1983 [10] Crowe C T. ASME Trans J Fluids Eng, 1982; 104: 297 [11] Ansys Inc. Ansys User's Manual. Pittsburgh, PA: Ansys Inc, 2004 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|