GRAIN BOUNDARY CHARACTER DISTRIBUTIONS OF Pb-Ca-Sn-Al ALLOY OF SOLUTION-TREATED AND PRE-AGED FOLLOWED BY STRAIN ANNEALING |
山东理工大学机械工程学院金属材料系 |
|
Cite this article:
. GRAIN BOUNDARY CHARACTER DISTRIBUTIONS OF Pb-Ca-Sn-Al ALLOY OF SOLUTION-TREATED AND PRE-AGED FOLLOWED BY STRAIN ANNEALING. Acta Metall Sin, 2007, 43(5): 454-458 .
|
Abstract The grain boundary character distributions (GBCD) of Pb-0.05%Ca-1.5%Sn-0.026%Al (mass fraction)alloy, which was solution treated at 290℃ and solution treated followed by pre-ageing at 100℃~200℃ prior to the same strain annealing, were investigated by means of electron back scatter diffraction ( EBSD) techniques. The results indicate that special boundaries were largely populated in the specimen which was strain annealed just after solution treatment. The fractions of ∑3 and(∑9+∑27)boundaries reached 49.6% and 7.2%, respectively, and the connectivity of general high angle boundaries (HABs) network was interrupted substantially by the special boundaries. However, special boundaries of fairly low fraction were developed in the specimen which was strain annealed after solution treatment and pre-ageing. The fractions of ∑3 and(∑9+∑27)boundaries was less than 35.9% and 2.5%, respectively, and the connectivity of general high angle boundaries (HABs) network was not interrupted significantly.
|
Received: 31 August 2006
|
|
[1] Palumbo G, Erb U. MRS Bull, 1999; 24(11): 27 [2] Lee D S, Ryoo H S, Hwang S K. Mater Sci Eng, 2003; A354: 106 [3] Xia S, Zhou B X, Chen W J, Wang W G. Ada Metall Sin, 2006; 42: 129 (夏爽,周邦新,陈文觉,王卫国.金属学报,2006;42:129) [4] Wang W G, Zhou B X, Feng L, Zhang X, Xia S. Acta Metall Sin, 2006; 42: 715 (王卫国,周邦新,冯柳,张欣,夏爽.金属学报,2006; 42:715) [5] Wang W G. Mater Sci Forum, 2007; 539-543: 3389 [6] Maitre A, Bourguignon G, Fiorani J M, Ghanbaja J, Steinmetz J. Mater Sci Eng, 2003; A358: 233 [7] Hilger J P. Power Sources, 1998; 72: 184 [8] Brandon D G. Acta Metall, 1966; 14: 1479 [9] Kaneno Y, Takasugi T. Mater Sci Eng, 2005; A393: 71 [10] Maitre A, Bourguignon G, Fiorani J M, J Steinmetz, Ghanbaja J. Mater Sci Eng, 2003; A340: 103 [11] Schuh C A, Kumar M, King W E. J Mater Sci, 2005; 40: 847 [12] Janssens K G F, Olmsted D, Holm E A, Foiles S M, Plimpton S J, Derlet P M. Nature Mater, 2006; 5: 124 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|