Electromaganic Wave Absorbing Property of Polyaniline / Polystylene Blends |
西北工业大学365所 |
|
Cite this article:
. Electromaganic Wave Absorbing Property of Polyaniline / Polystylene Blends. Acta Metall Sin, 2007, 43(4): 409-412 .
|
Abstract The electromaganic wave absorbing property of Polyaniline (PAni) / Polystylene (PS) blends were studied. The results indicated that The conductivity and electromagnetic wave absorbing property of PAni/PS blends increased with the increasing content of the doped PAni. Doped PAni with fibrous morphology had better electromagnetic wave absorbing property than that of PAni with nonfibrous morphology. The frequency breadth of the reflectivity below -10dB was 6GHz(11.6~17.6 GHz)by optimization of the electromaganic parameters of the PAni/ PS micro/nano-blend.
|
Received: 21 June 2006
|
|
[1]Psilopoulos J,Gruber J.Microwave Opt Technol Lett, 2001;30:254 [2]Zhao J P,Li Y,Wu P L.Mater Sci Technol,2002;10:219 (赵九蓬,李直,吴佩莲.材料科学与工艺,2002;10:219) [3]Heeger A J.Rev Mod Phys,2001;73:681 [4]Olmedo L.Hourquebie P,Jousse F.Synth Met,1995;65: 205 [5]Wan M X,Li J C,Li S Z.Polym Adv Technol,2001;12: 651 [6]Vinoy K J,Jha R M.Sāddhanā,1995;20:815 [7]Xing L Y.Stealing Materials.Beijing:Chemical Industry ??Press,2004:82 (邢丽英.隐身材料.北京:化学工业出版社,2004:82) [8]Courric S,Tran V H.J Polym Adv Technol,2000;11:273 [9]Wan M X,Li S Z,Li J C,Chao Y.Aerosp Mater Technol, 1989;(4):28 (万梅香,李素珍,李军朝,曹镛.宇航工艺材料,1989;(4): 28) [10]Liao H X,Liu Z L,Yu G X.J Cent Chin Norm Univ[Nat Sci),2004;38:340 (廖海星,刘祖黎,喻古雄.华中师范大学学报(自然科学版), 2004;38:340) [11]Coltevieille D,Le MéhautéA,Challioui C.Mirebeau P, Demay J N.Synth Met,1999;101:703 [12]Ge F D,Zhu J,Chen L M.Aerosp Mater Technol,1996; (5):42 (葛副鼎,朱静,陈利民.宇航材料工艺,1996;(5):42) [13]Guo X M.PhD Dissertation,Institute of Metal Research, Chinese Academy of Sciences,Shenyang,2005 (郭雪梅.中国科学院金属研究所博士学位论文,沈阳,2005) [14]Kang Q.Novel Microwave Absorbing Materials.Beijing: Science Press,2005:66 (康青.新型微波吸收材料.北京:科学出版社,2005:66) [15]Zou Y,Wang G Q,Liao H X,Liu Z L.J Huazhong Univ Sci Technol(Nat Sci),2001;29:87 (邹勇,王国强,廖海星,刘祖黎.华中科技大学学报,2001; 29:87) |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|