Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (4): 409-412     DOI:
Research Articles Current Issue | Archive | Adv Search |
Electromaganic Wave Absorbing Property of Polyaniline / Polystylene Blends
西北工业大学365所
Cite this article: 

. Electromaganic Wave Absorbing Property of Polyaniline / Polystylene Blends. Acta Metall Sin, 2007, 43(4): 409-412 .

Download:  PDF(687KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The electromaganic wave absorbing property of Polyaniline (PAni) / Polystylene (PS) blends were studied. The results indicated that The conductivity and electromagnetic wave absorbing property of PAni/PS blends increased with the increasing content of the doped PAni. Doped PAni with fibrous morphology had better electromagnetic wave absorbing property than that of PAni with nonfibrous morphology. The frequency breadth of the reflectivity below -10dB was 6GHz(11.6~17.6 GHz)by optimization of the electromaganic parameters of the PAni/ PS micro/nano-blend.
Key words:  Polyaniline      Polystylene      micro/nano-blend      doping      electromaganic wave absorbing property      
Received:  21 June 2006     
ZTFLH:  TB332  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I4/409

[1]Psilopoulos J,Gruber J.Microwave Opt Technol Lett, 2001;30:254
[2]Zhao J P,Li Y,Wu P L.Mater Sci Technol,2002;10:219 (赵九蓬,李直,吴佩莲.材料科学与工艺,2002;10:219)
[3]Heeger A J.Rev Mod Phys,2001;73:681
[4]Olmedo L.Hourquebie P,Jousse F.Synth Met,1995;65: 205
[5]Wan M X,Li J C,Li S Z.Polym Adv Technol,2001;12: 651
[6]Vinoy K J,Jha R M.Sāddhanā,1995;20:815
[7]Xing L Y.Stealing Materials.Beijing:Chemical Industry ??Press,2004:82 (邢丽英.隐身材料.北京:化学工业出版社,2004:82)
[8]Courric S,Tran V H.J Polym Adv Technol,2000;11:273
[9]Wan M X,Li S Z,Li J C,Chao Y.Aerosp Mater Technol, 1989;(4):28 (万梅香,李素珍,李军朝,曹镛.宇航工艺材料,1989;(4): 28)
[10]Liao H X,Liu Z L,Yu G X.J Cent Chin Norm Univ[Nat Sci),2004;38:340 (廖海星,刘祖黎,喻古雄.华中师范大学学报(自然科学版), 2004;38:340)
[11]Coltevieille D,Le MéhautéA,Challioui C.Mirebeau P, Demay J N.Synth Met,1999;101:703
[12]Ge F D,Zhu J,Chen L M.Aerosp Mater Technol,1996; (5):42 (葛副鼎,朱静,陈利民.宇航材料工艺,1996;(5):42)
[13]Guo X M.PhD Dissertation,Institute of Metal Research, Chinese Academy of Sciences,Shenyang,2005 (郭雪梅.中国科学院金属研究所博士学位论文,沈阳,2005)
[14]Kang Q.Novel Microwave Absorbing Materials.Beijing: Science Press,2005:66 (康青.新型微波吸收材料.北京:科学出版社,2005:66)
[15]Zou Y,Wang G Q,Liao H X,Liu Z L.J Huazhong Univ Sci Technol(Nat Sci),2001;29:87 (邹勇,王国强,廖海星,刘祖黎.华中科技大学学报,2001; 29:87)
[1] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[2] MAO Fei, LU Hao, TANG Fawei, GUO Kai, LIU Dong, SONG Xiaoyan. First-Principle Calculation on the Effect of Mn and In on the Structural Stability and Magnetic Moment of SmCo7 Alloys[J]. 金属学报, 2021, 57(7): 948-958.
[3] Shasha YANG,Feng YANG,Minghui CHEN,Yunsong NIU,Shenglong ZHU,Fuhui WANG. Effect of Nitrogen Doping on Microstructure and Wear Resistance of Tantalum Coatings Deposited by Direct Current Magnetron Sputtering[J]. 金属学报, 2019, 55(3): 308-316.
[4] Chengyang JIANG, Yingfei YANG, Zhengyi ZHANG, Zebin BAO, Shenglong ZHU, Fuhui WANG. Preparation and Enhanced Hot Corrosion Resistance of aZr-Doped PtAl2+(Ni, Pt)Al Dual-Phase Coating[J]. 金属学报, 2018, 54(4): 581-590.
[5] Shizheng ZHANG,Yaohui XU,Tingyu WANG,Ruixing LI,Hongnian CAI. SOLID SOLUBILITY AND OXYGEN STORAGE CAPABILITY OF In3+-DOPED CeO2[J]. 金属学报, 2016, 52(5): 607-613.
[6] LI Honglin, ZHANG Zhong, LU Yingbo, HUANG Jinzhao, LIU Ruxi. FIRST-PRINCIPLES AND EXPERIMENTAL STUDY ON THE ELECTRONIC AND OPTICAL PROPERTIES OF Eu DOPED ZnO STRUCTURE[J]. 金属学报, 2013, 29(4): 506-512.
[7] ZHOU Liying, WANG Fuhe. FIRST-PRINCIPLES STUDY OF EFFECT OF POINT DEFECT ON ADSORPTION AND DIFFUSION OF OXYGEN AT γ-TiAl (100) SURFACE[J]. 金属学报, 2013, 49(11): 1387-1391.
[8] LI Ying, DING Yushi, CUI Shaogang, WANG Changzhen. PREPARATION AND ELECTRICAL PROPERTIES OF Sc--DOPED CaZrO3[J]. 金属学报, 2012, 48(5): 575-578.
[9] SANG Xiaoguang, ZENG Fanwu, LIU Xiaoxia. ELECTROCHEMICAL PREPARATION OF PANI/CeO2 COMPOSITE WITH SPECIAL MORPHOLOGY[J]. 金属学报, 2012, 48(4): 508-512.
[10] FAN Yongzhong ZHANG Shujuan TU Jinwei SUN Xia LIU Fang LI Mingsheng. INFLUENCE OF DOPING WITH Si AND Y ON STRUCTURE AND PROPERTIES OF (Ti, Al)N COATING[J]. 金属学报, 2012, 48(1): 99-106.
[11] LI Ying MA Beiyue WANG Zhenming JIANG Maofa. PREPARATION OF Na1.4Co2O4 BASED THERMOELECTRIC MATERIALS BY SOL-GEL METHOD AND CHARACTERIZATION[J]. 金属学报, 2011, 47(1): 109-114.
[12] XIANG Xin CHEN Chang'an LIU Kezhao LUO Lizhu LIU Tingting WANG Xiaoying. EFFECT OF C DOPING ON He BEHAVIOR IN Al[J]. 金属学报, 2010, 46(3): 318-323.
[13] YANG Yiyong PENG Zhijian FU Zhiqiang WU Sudong CHEN Xinchun WANG Chengbiao. STUDY ON W GRADED DOPING DLC COMPOSITE FILMS WITH MULTICOMPONENT TRANSITION LAYER[J]. 金属学报, 2010, 46(1): 34-40.
[14] ZHANG Xia WANG Jing CHEN Li. STRUCTURE AND PERFORMANCE OF Fe2O3-PANI COMPOSITE NANOPARTICLES SYNTHESIZED BY ELECTROSTATIC SELF-ASSEMBLY[J]. 金属学报, 2009, 45(9): 1135-1140.
[15] ZHANG Jingyu LIU Qingfeng LIU Qian. EFFECT OF Ti ON THE ANTI-CORROSION PROPERTY OF Zn-Al ALLOY FILMS[J]. 金属学报, 2009, 45(10): 1166-1170.
No Suggested Reading articles found!