| Numerical Simulation of two-phase Solidification Process of |
| 大连理工大学三束材料改性国家重点实验室及材料学院 |
|
Cite this article:
. Numerical Simulation of two-phase Solidification Process of. Acta Metall Sin, 2007, 43(6): 668-672 .
|
|
|
Abstract In this paper, the two-phase model of globular equiaxed grain solidification has been used to compute the solidification process of Sn-3.5%Pb hollow billet under traveling magnetic field. The temperature gradient, cooing rate, solute concentration distribution and grain size are studied under different stirring velocities. The results show that the traveling magnetic field can result in a global circulation flow in the molten metal, the temperature field is uniformed and the grain size is refined which improve the solidification structure of hollow billet. However, the macro segregation is produced in the hollow billet by the forced flow. So, the stirring velocity should be controlled carefully during the casting of hollow billets.
|
|
Received: 10 October 2006
|
|
|
[1]Wang Z F,Cui J Z,Yang Y S,Zheng H.Acta Metall Sin, 2006;42:317 (王哲峰,崔建忠,杨院生,郑辉.金属学报,2006;42:317) [2]Wang Z F,Cui J Z,Piao F X.Chin J Nonferrous Met, 2006;16:500 (王哲峰,崔建忠,朴凤贤.中国有色金属学报,2006;16:500) [3]Li Q L,Li T J,Jin J Z.Mater Sci Technol,2003;11:148 (李丘林,李廷举,金俊泽.材料科学与工艺,2003;11:148) [4]Zhang Q,Li T J,Wang T M,Jin J Z.Rare Met Mater Eng,2007,in press (张琦,李廷举,王同敏,金俊泽.稀有金属材料与工程,2007,待发表) [5]Oszk B,Preis K.Metall Trans,1985;16B:377 [6]Biro O.IEEE Trans Magn,1988;24:102 [7]Feng C Z.Electromagnetic Field.Beijing:People Educa- tion Press,1985:279 (冯慈璋.电磁场.北京:人民教育出版社,1985:279) [8]Wang T M,Yao S,Zhang X G,Jin J Z,Wu M,Ludwig A,Pustal B,Buhrig-Polaczek A.Acta Metall Sin,2006; 42:584 (王同敏,姚山,张兴国,金俊泽,Wu M,Ludwig A,Pustal B,Buhrig-Polaczek A.金属学报,2006;42:584) [9]Wu X L,Wang F M,Huang X X,Li Y,Zhu Y M.Steel- making,2005;21(5):21 (吴小林,王福明,黄晓星,李英,祝宜明.炼钢,2005;21(5): 21) [10]Li Y M,Ai X L.Foundry,2002;51:756 (李英民,艾秀兰.铸造,2002;51:756) [11]Willers B,Eckert S,Michel U,Haase I,Zouhar G.Mater Sci Eng,2005;A402:55 [12]Eckert S,Willers B,Nikrityuk P A,Eckert K,Michel U, Zouhar G.Mater Sci Eng,2005;A413-414:211 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|