Numerical Simulation of two-phase Solidification Process of
大连理工大学三束材料改性国家重点实验室及材料学院
Cite this article: 

. Numerical Simulation of two-phase Solidification Process of. Acta Metall Sin, 2007, 43(6): 668-672 .

Download:  PDF(448KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In this paper, the two-phase model of globular equiaxed grain solidification has been used to compute the solidification process of Sn-3.5%Pb hollow billet under traveling magnetic field. The temperature gradient, cooing rate, solute concentration distribution and grain size are studied under different stirring velocities. The results show that the traveling magnetic field can result in a global circulation flow in the molten metal, the temperature field is uniformed and the grain size is refined which improve the solidification structure of hollow billet. However, the macro segregation is produced in the hollow billet by the forced flow. So, the stirring velocity should be controlled carefully during the casting of hollow billets.
Key words:  traveling magnetic field      hollow billet      temperature field      concentration field      
Received:  10 October 2006     
ZTFLH:  TG29  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I6/668

[1]Wang Z F,Cui J Z,Yang Y S,Zheng H.Acta Metall Sin, 2006;42:317 (王哲峰,崔建忠,杨院生,郑辉.金属学报,2006;42:317)
[2]Wang Z F,Cui J Z,Piao F X.Chin J Nonferrous Met, 2006;16:500 (王哲峰,崔建忠,朴凤贤.中国有色金属学报,2006;16:500)
[3]Li Q L,Li T J,Jin J Z.Mater Sci Technol,2003;11:148 (李丘林,李廷举,金俊泽.材料科学与工艺,2003;11:148)
[4]Zhang Q,Li T J,Wang T M,Jin J Z.Rare Met Mater Eng,2007,in press (张琦,李廷举,王同敏,金俊泽.稀有金属材料与工程,2007,待发表)
[5]Oszk B,Preis K.Metall Trans,1985;16B:377
[6]Biro O.IEEE Trans Magn,1988;24:102
[7]Feng C Z.Electromagnetic Field.Beijing:People Educa- tion Press,1985:279 (冯慈璋.电磁场.北京:人民教育出版社,1985:279)
[8]Wang T M,Yao S,Zhang X G,Jin J Z,Wu M,Ludwig A,Pustal B,Buhrig-Polaczek A.Acta Metall Sin,2006; 42:584 (王同敏,姚山,张兴国,金俊泽,Wu M,Ludwig A,Pustal B,Buhrig-Polaczek A.金属学报,2006;42:584)
[9]Wu X L,Wang F M,Huang X X,Li Y,Zhu Y M.Steel- making,2005;21(5):21 (吴小林,王福明,黄晓星,李英,祝宜明.炼钢,2005;21(5): 21)
[10]Li Y M,Ai X L.Foundry,2002;51:756 (李英民,艾秀兰.铸造,2002;51:756)
[11]Willers B,Eckert S,Michel U,Haase I,Zouhar G.Mater Sci Eng,2005;A402:55
[12]Eckert S,Willers B,Nikrityuk P A,Eckert K,Michel U, Zouhar G.Mater Sci Eng,2005;A413-414:211
[1] TANG Haiyan, LI Xiaosong, ZHANG Shuo, ZHANG Jiaquan. Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control[J]. 金属学报, 2020, 56(12): 1629-1642.
[2] Xinhua LIU, Huadong FU, Xingqun HE, Xintong FU, Yanqing JIANG, Jianxin XIE. Numerical Simulation Analysis of Continuous Casting Cladding Forming for Cu-Al Composites[J]. 金属学报, 2018, 54(3): 470-484.
[3] Xiaoyu CHONG, Guangchi WANG, Jun DU, Yehua JIANG, Jing FENG. Numerical Simulation of Temperature Field and Thermal Stress in ZTAp/HCCI Composites DuringSolidification Process[J]. 金属学报, 2018, 54(2): 314-324.
[4] Yadong CHEN, Yunrong ZHENG, Qiang FENG. EVALUATING SERVICE TEMPERATURE FIELD OF HIGH PRESSURE TURBINE BLADES MADE OF DIRECTIONALLY SOLIDIFIED DZ125 SUPERALLOY BASED ON MICRO-STRUCTURAL EVOLUTION[J]. 金属学报, 2016, 52(12): 1545-1556.
[5] ZHAO Bo, WU Chuansong,JIA Chuanbao, YUAN Xin. NUMERICAL ANALYSIS OF THE WELD BEAD PROFILES IN UNDERWATER WET FLUX-CORED ARC WELDING[J]. 金属学报, 2013, 49(7): 797-803.
[6] XU Qingdong, LIN Xin, SONG Menghua, YANG Haiou, HUANG Weidong. MICROSTRUCTURE OF HEAT-AFFECTED ZONE OF LASER FORMING REPAIRED 2Cr13 STAINLESS STEEL[J]. 金属学报, 2013, 49(5): 605-613.
[7] PANG Ruipeng, WANG Fuming, ZHANG Guoqing, LI Changrong. STUDY OF SOLIDIFICATION THERMAL PARAMETERS OF 430 FERRITE STAINLESS STEEL BASED ON 3D-CAFE METHOD[J]. 金属学报, 2013, 49(10): 1234-1242.
[8] KE Changbo, CAO Shanshan, MA Xiao, HUANG Ping, ZHANG Xinping. PHASE FIELD SIMULATION OF AUTO-CATALYTIC GROWTH EFFECT OF COHERENT Ni4Ti3 PRECIPITATE IN NiTi SHAPE MEMORY ALLOY[J]. 金属学报, 2013, 49(1): 115-122.
[9] CHEN Zhihui WANG Engang ZHANG XingwuWANG Yuanhua ZHU Mingwei HE Jicheng. STUDY ON THE BEHAVIOUR OF BUBBLES IN A CONTINUOUS CASTING MOLD WITH Ar INJECTION AND TRAVELING MAGNETIC FIELD[J]. 金属学报, 2012, 48(8): 951-956.
[10] WEI Jie DONG Junhua KE Wei. NUMERICAL SIMULATION AND EXPERIMENTAL STUDY ON TEMPERATURE FIELD DURING CHEMICAL REAGENT COOLING PROCESS OF HOT ROLLED REBAR[J]. 金属学报, 2012, 48(1): 115-121.
[11] FENG Mingjie WANG Engang HE Jicheng. NUMERICAL SIMULATION ON TEMPERATURE FIELD IN HIGH SPEED STEEL COMPOSITE ROLL DURING CONTINUOUS POURING PROCESS FOR CLADING I. Graphite Mould Method[J]. 金属学报, 2011, 47(12): 1495-1502.
[12] FENG Mingjie WANG Engang HE Jicheng. NUMERICAL SIMULATION ON TEMPERATURE FIELD IN HIGH SPEED STEEL COMPOSITE ROLL DURING CONTINUOUS POURING PROCESS FOR CLADDING
II. Copper Mould Method
[J]. 金属学报, 2011, 47(12): 1503-1512.
[13] LI Baokuan DAI Fengyu QI Fengsheng YANG Ran. FLOW FIELD AND CONCENTRATION FIELD OF ALLOYING ADDITION IN CLAD STEEL CONTINUOUS CASTING MOLD USING LONG AND SHORT NOZZLES[J]. 金属学报, 2010, 46(6): 736-742.
[14] YU Haiqi ZHU Miaoyong. 3-D NUMERICAL SIMULATION OF FLOW FIELD AND TEMPERATURE FIELD IN A ROUND BILLET CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC STIRRING[J]. 金属学报, 2008, 44(12): 1465-1473.
[15] Qiaodan Hu; Peng Luo; Jianguo Li. FINITE ELEMENT MODELING OF TEMPERATURE DISTRIBUTION IN FIELD ACTIVATED SINTERING OF MoSi2-SiC COMPOSITE[J]. 金属学报, 2008, 44(10): 1253-1259 .
No Suggested Reading articles found!