Abstract The Fe containing phase in
hypereutectic Al-2.89%Fe alloy was accumulated towards the
sample center under the alternating magnetic field, which is due to a
large compression force orientated the sample axis acted on Al3Fe
phases with a large magnetic susceptibility than melt aluminium. X-ray
diffraction results showed that there was only Al3Fe phase existing
in the Fe containing phases, whether solidified with or without
the AC magnetic field. The alternating magnetic field can affect the
distribution of the Fe containing phase instead of their type.
|
Received: 18 October 2005
|
|
[1] Gillon P. Mater Sci Eng, 2000; A287: 146 [2] Asai S. Sci Technol Adv Mater, 2000; 1: 191 [3] Radjai A, Miwa K. Metall Mater Trans, 2002; 33A: 3025 [4] Zhang J, Tan Y Y, Li S M. Sci Technol Adv Mater, 2001; 2: 205 [5] Liu X F, Bian X F, Liu Y X, Zhang G H, Ma J J. Acta Metall Sin, 1997; 33: 1062 (刘相法,边秀房,刘玉先,张国华,马家骥.金属学报,1997; 33:1062) [6] Parkhutik P A, Kalinichenko A S, Kupriyanova I Yu, Chebotko L S, Antonevich M A, Savitskaya Ye V. Phys Met Metallogr, 1990; 70: 151 [7] Lu L, Dahle A K. Metall Mater Trans, 2005; 36A: 819 [8] Zhou Z P, Ma J C, Bai Y H, Yu H P, Li R D. Foundry, 2002; 51: 343 (周振平,马建超,白彦华,于海朋,李荣德.铸造,2002;51: 343) [9] Li R D, Ma J C, Zhou Z P. Hot Work Technol, 2004; (4): 14 (李荣德,马建超,周振平.热加工工艺, 2004;(4):14) [10] Liu P, Thorvaldsson T, Dunlop G L. Mater Sci Technol, 1986; 2: 1009 [11] Mondolfo L F. Aluminum Alloys: Structure and Properties. London: The Whitefriars Press Ltd, 1976: 284, 88 |