Acta Metall Sin  2006, Vol. 42 Issue (4): 355-360     DOI:
Research Articles Current Issue | Archive | Adv Search |
Preparation and Protection of Al Diffusion Coatings on gama-TiAl
中科院金属所
Cite this article: 

. Preparation and Protection of Al Diffusion Coatings on gama-TiAl. Acta Metall Sin, 2006, 42(4): 355-360 .

Download:  PDF(937KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Al diffusion coatings were prepared on g-TiAl alloy by first arc ion plant Al then interdiffusion treatment processes. Al diffusion coatings have a good adherence with the substrate, and EDX and XRD show that the coatings composed of outer thick layer TiAl3 and inner thin layer TiAl2. For g-TiAl without coating under high temperature oxidation at 900oC in air, multilayer oxide scale is formed and consisted of mix of TiO2 and Al2O3, which exhibits relatively poor oxidation resistance. The high temperature oxidation resistance of the specimens coated with Al diffusion coatings is remarkably improved due to the formation of a dense and adherent Al2O3 scale. The oxidation and degradation mechanism of Al diffusion coatings also are discussed.
Key words:       
Received:  15 August 2005     
ZTFLH:  TG146.2  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I4/355

[1] Clemens H, Lorich A, Eberhardt N, Glatz W, Knabl W, Kestler H. Z Metallkd, 1999; 90: 569
[2] Wu X H, Hu D, Loretto M H. J Mater Sci, 2004; 39: 3935
[3] Williams J C. Proc JISSE-5, SAMPE, Tokyo, Japan, 1997: 1153
[4] Noda T. Intermetallics, 1998; 6: 709
[5] Brady M P, Brindley W J, Smialek J L, Locci I E. JOM, 1997: 46
[6] Munro T C, Gleeson B. Metall Mater Trans, 1996; 27A: 3761
[7] Nishimotoa T, Izumia T, Hayashib S, Naritab T. Intermetallics, 2003; 11: 225
[8] Swadzba L, Moskal G, Hetmanczyk M, Mendala B, Jar- czyk G. Surf Coat Technol, 2004; 184: 93
[9] Tang Z L, Wang F H, Wu W T. Surf Coat Technol, 1998; 99: 248
[10] Lee J K, Oh M H, Lee H K, Wee D M. Surf Coat Technol, 2004; 182: 363
[11] Singheiser L, Niewolak L, Flesch U, Shemet V, Quadakkers W J. Metall Mater Trans, 2003; 34A: 2247
[12] Guo M H, Wang Q M, Ke P L, Cui Y Y, Gong J, Sun C, Wen L S. Ada Metall Sin, 2005; 41: 312 (郭明虎,王启民,柯培玲,崔玉友,宫骏,孙超,闻立时. 金属学报,2005;41:312)
[13] Chu M S, Wu S K. Acta Mater, 2003; 51: 3109
[14] Murray J L. Phase Diagrams of Binary Titanium Alloys. Materials Park, Ohio: ASM International, 1987: 225
[15] van Loo F J J, Rieck G D. Acta Metall, 1973; 21: 73
[16] Eckert M, Bencze L, Kath D, Nickel H, Hilpert K. Phys Chem, 1996; 100: 418
[17] Becker S, Rahmel A, Schorr M, Schutze M.Oxid Met, 1992; 38: 425
[18] Li X L, Hillel R, Teyssandier F, Choi S K, van Loo F J J. Acta Metall Mater, 1992; 40: 3149
[19] Chen Y, Young D J, Gleeson B. Mater Lett, 1995; 22: 125
[20] Rakowski J M, Pettit F S, Meier G H, Dettenwanger F, Schumann E, Ruhle M. Scr Metall Mater, 1995; 33: 997
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!