| Effects of Al Interlayer and Ni(V) Transition Layer on the Welding Residual Stress of Co/Al/Cu Sandwich Target Assembly |
JIANG Lin1,2, ZHANG Liang1,3, LIU Zhiquan1,2,4( ) |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China 3 School of Mechatronic Engineering, Jiangsu Normal University, Xuzhou 221116, China 4 Shenzhen Institute of Advanced Electronic Materials, Shenzhen Institutes of Advanced Technology, Chinese Academy of Sciences, Shenzhen 518055, China |
|
Cite this article:
JIANG Lin, ZHANG Liang, LIU Zhiquan. Effects of Al Interlayer and Ni(V) Transition Layer on the Welding Residual Stress of Co/Al/Cu Sandwich Target Assembly. Acta Metall Sin, 2020, 56(10): 1433-1440.
|
|
|
Abstract Sputtering has been widely used to prepare thin film due to its good cohesion with substrate, high purity, compactness, repeatability and large area manufacture. Target is a key consumable material during production of thin film by sputtering. Generally, targets are mostly rare and high purity metal, so the cost of target is very high. In order to reduce the cost of target, to improve its stiffness, and to enhance the electrical and thermal conductivity, target is usually connected with backplane to form the target assembly. The main connection method is diffusion welding, which is used in the industrial production. However, the target and the backplane are usually two different materials with different physical properties such as coefficient of thermal expansion (CTE) and thermal conductivity. During the welding or soldering process of target, the mismatch of physical properties will lead to residual stress in target, which has a direct influence on the thickness and microstructure uniformity of the films. Hence, it is very meaningful to investigate the residual stress in target and to study its influencing factor. Based on the Co/Al/Cu sandwich structure of backplane diffusion welding, the effects of Al interlayer and Ni(V) layer on welding residual stress were studied by finite element method. It was found that the application of the Al interlayer not only can make diffusion welding process easier and lower the diffusion welding temperature, but also can reduce the maximum residual stress from 142 MPa to 126 MPa. Furthermore, the location of the maximum residual stress also changes from the outer edge of the interface between target and backplane to the position near the symmetrical axis of target and Co/Al interface. Furthermore, there is an optimal thickness for Al interlayer (7 mm). Although the existence of Ni(V) layer can inhibit the generation of brittle intermetallic compounds at the interface of Co/Al and Cu/Al, it also increases the residual stress. Moreover, we find that the increase of residual stress with Ni(V) layer at only Co/Al interface, is smaller than that of adding Ni(V) layer at both Co/Al and Cu/Al interfaces.
|
|
Received: 24 February 2020
|
|
|
| Fund: National Key Research and Development Program of China(2017YFB0305501) |
| [1] |
Martens S, Mack W, Courtade F, et al. Laser-based target preparation in 3D integrated electronic packages [J]. J. Electron. Packag., 2009, 131: 031006
doi: 10.1115/1.3144157
|
| [2] |
Huang D S, Tu W B, Zhang X M, et al. Using Taguchi method to obtain the optimal design of heat dissipation mechanism for electronic component packaging [J]. Microelectron. Reliab., 2016, 65: 131
|
| [3] |
Huang M L, Yang F. Size effect model on kinetics of interfacial reaction between Sn-xAg-yCu solders and Cu substrate [J]. Sci. Rep., 2014, 4: 7117
|
| [4] |
Takahashi K, Hoshino M, Yonemura H, et al. Development of advanced 3D chip stacking technology with ultra-fine interconnection [A]. 2001 Proceedings. 51st Electronic Components and Technology Conference [C]. Orlando, FL, USA: IEEE, 2001: 541
|
| [5] |
Ge Z P, Wang K K. Optimization of structure for BGA packaging based on Taguchi method [A]. 2015 16th International Conference on Electronic Packaging Technology (ICEPT) [C]. Changsha: IEEE, 2015: 1433
|
| [6] |
Lai L F, Wang J X, Wang H T, et al. Structures and properties of C-doped NiCr thin film deposited by closed-field unbalanced magnetron sputtering [J]. J. Electron. Mater., 2017, 46: 552
|
| [7] |
Lin Y P, Hsieh T E, Chen Y C, et al. Characteristics of Cu2ZnSn (SxSe1-x)4 thin-film solar cells prepared by sputtering deposition using single quaternary Cu2ZnSnS4 target followed by selenization/sulfurization treatment [J]. Sol. Energy Mater. Sol. Cells, 2017, 162: 55
|
| [8] |
Shih C W, Chin A, Lu C F, et al. Remarkably high hole mobility metal-oxide thin-film transistors [J]. Sci. Rep., 2018, 8: 889
|
| [9] |
Zeng Y, Liang G X, Fan P, et al. The structural, optical and thermoelectric properties of single target sputtered Cu2-ZnSn-(S, Se)4 thin film [J]. J. Mater. Sci.: Mater. Electron., 2017, 28: 13763
|
| [10] |
Ling Q. Investigation of manufacture of TiO2 target (Nb2O5) and its performance [D]. Shenzhen: Shenzhen University, 2017
|
|
(凌 奇. Nb2O5掺杂TiO2靶材的制备及性能的研究 [D]. 深圳: 深圳大学, 2017)
|
| [11] |
Zhao B H, Fan H B, Sun Y J. Molybdenum sputtering film and target for TFT-LCD manufacture [J]. China Molybd. Ind., 2011, 35(1): 7
|
|
(赵宝华, 范海波, 孙院军. TFT-LCD制造用钼薄膜溅射及其靶材 [J]. 中国钼业, 2011, 35(1): 7)
|
| [12] |
Yang B C, Cui H L. Manufacture and application of sputtering target materials [J]. Vacuum, 2001, (3): 11
|
|
(杨邦朝, 崔红玲. 溅射靶材的制备与应用 [J]. 真空, 2001, (3): 11)
|
| [13] |
Jiang L, Zhang L, Liu Z Q. Optimal design of Co/In/Cu sputtering target assembly using finite element method and Taguchi method [J]. Acta Metall. Sin. (Engl. Lett.), 2019, 32: 1407
|
| [14] |
Shah R P, Steele D E, Turner W R, et al. Ni-plated target diffusion bonded to a backing plate and method of making same [P]. PU.S. at, 6555250, 2003
|
| [15] |
Zhu R D, Dong W C, Lin H Q, et al. Finite element simulation of welding residual stress for buffer beam of CRH2A high speed train [J]. Acta Metall. Sin., 2014, 50: 944
|
|
(朱瑞栋, 董文超, 林化强等. CRH2A 型动车组缓冲梁结构焊接残余应力的有限元模拟 [J]. 金属学报, 2014, 50: 944)
|
| [16] |
Kovalev S P, Miranzo P, Osendi M I. Finite element simulation of thermal residual stresses in joining ceramics with thin metal interlayers [J]. J. Am. Ceram. Soc., 1998, 81: 2342
|
| [17] |
Zhang Z G, Qi B Y, Jin Z W, et al. Perylene diimides: A thickness-insensitive cathode interlayer for high performance polymer solar cells [J]. Energy Environ. Sci., 2014, 7: 1966
|
| [18] |
Ali R, Sebastiani M, Bemporad E. Influence of Ti-TiN multilayer PVD-coatings design on residual stresses and adhesion [J]. Mater. Des., 2015, 75: 47
|
| [19] |
Lee I H, Kim T G, Park Y. Growth of crack-free AlGaN film on high-temperature thin AlN interlayer [J]. J. Cryst. Growth, 2002, 234: 305
doi: 10.1016/S0022-0248(01)01702-X
|
| [20] |
Lin C R, Kuo C T, Chang R M. Improvement in adhesion of diamond films on cemented WC substrate with Ti-Si interlayers [J]. Diam. Relat. Mater., 1998, 7: 1628
|
| [21] |
Wang B L, Li Y Z, Huo Y Z. Thermal stress distributions and optimization on stress reductions with or/and without linearly graded interlayers [J]. Composites, 2011, 42B: 993
|
| [22] |
Liu C Y, Tu K N, Sheng T T, et al. Electron microscopy study of interfacial reaction between eutectic SnPb and Cu/Ni(V)/Al thin film metallization [J]. J. Appl. Phys., 2000, 87: 750
|
| [23] |
Jang G Y, Duh J G. Elemental redistribution and interfacial reaction mechanism for the flip chip Sn-3.0Ag-(0.5 or 1.5)Cu solder bump with Al/Ni(V)/Cu under-bump metallization during aging [J]. J. Electron. Mater., 2006, 35: 2061
|
| [24] |
Resnik D, Vrtačnik D, Aljančič U, et al. Influence of mechanical stress on adhesion properties of DC magnetron sputtered Ti/NiV/Ag layers on n+ Si substrate [J]. Microelectron. Eng., 2008, 85: 1603
|
| [25] |
Li R F, Chen H N, Yu L, et al. GB/T 31218-2014 Metallic materials—Determination of residual stress—Sectioning relaxation strain-gage method [S]. Beijing: China Standard Press, 2015
|
|
(李荣锋, 陈怀宁, 余 立等. GB/T 31218-2014 金属材料 残余应力测定 全释放应变法 [S]. 北京: 中国标准出版社, 2015)
|