EFFECT OF HYDROSTATIC PRESSURE AND PRE-STRESS ON CORROSION BEHAVIOR OF A NEW TYPE Ni-Cr-Mo-V HIGH STRENGTH STEEL
Lin FAN,Kangkang DING,Weimin GUO,Penghui ZHANG,Likun XU()
State Key Laboratory for Marine Corrosion and Protection, Luoyang Ship Material Research Institute, Qingdao 266101, China
Cite this article: 

Lin FAN,Kangkang DING,Weimin GUO,Penghui ZHANG,Likun XU. EFFECT OF HYDROSTATIC PRESSURE AND PRE-STRESS ON CORROSION BEHAVIOR OF A NEW TYPE Ni-Cr-Mo-V HIGH STRENGTH STEEL. Acta Metall Sin, 2016, 52(6): 679-688.

Download:  HTML  PDF(1527KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The efforts on deep sea exploration and development have posed many challenges on the corrosion resistance and safety use of high strength steel in recent years. This has attracted a lot of attentions on the corrosion behavior of high strength steel in deep sea environment. Hydrostatic pressure has been identified as one of the most significant factors that affect pitting corrosion of materials or steel structures used in deep sea. However, pre-stress introduced by the actual service conditions is probably another critical factor of deep sea corrosion. The purpose of this work is to investigate the corrosion behavior of a new type Ni-Cr-Mo-V high strength steel under the combined stresses of hydrostatic pressure and preloaded tensile stress in simulated deep-sea environment. Corrosion rate measurement, SEM observation, statistical analysis of pitting geometry and finite element (FE) analysis were used in this work. The results indicated that corrosion rate of Ni-Cr-Mo-V high strength steel increased with the increase of hydrostatic pressure and pre-stress. The deterioration of corrosion resistance of the steel mainly reflected in pit initiation, pit growth and pit coalescence. Rather than pre-stress, hydrostatic pressure exhibited obvious effect on promoting pit initiation. Pits initiated in the form of corrosion pin-holes, which randomly distributed at the corroded surface. Both hydrostatic pressure and pre-stress facilitated pit growth, and there was an interaction between them, which was more remarkable at higher pre-stress. Hydrostatic pressure was mainly responsible for pit growth parallel to the steel surface, while pre-stress was essential to pit depth increase. Adjacent pits were inclined to coalesce in the direction perpendicular to pre-stress. With the increase of hydrostatic pressure and pre-stress, the aspect ratio of pits increased, which can lead to the formation of uniform corrosion.

Key words:  high strength steel      hydrostatic pressure      pre-stress      deep-sea environment      pitting     
Received:  11 November 2015     

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2015.00577     OR     https://www.ams.org.cn/EN/Y2016/V52/I6/679

Fig.1  Schematics of experimental setup (a) and tensile stress preloading device with specimen (b) (1—solution tank, 2—piston pump, 3—valve, 4—cooling equipment, 5—temperature/pressure monitor, 6—thermocouple, 7—pre-stress loading device, 8—pressure sensor)
Fig.2  

Relationships between corrosion rate (D1~D4) of Ni-Cr-Mo-V high strength steel and pre-stress (σ) after 168 h immersion in simulated deep-sea environment (5 ℃, 3.5%NaCl) at different hydrostatic pressures

Fig.3  Relationships between measured (a) and calculated (b) corrosion rates of Ni-Cr-Mo-V high strength steel and hydrostatic pressure and pre-stress
Fig.4  Plot show corrosion rate of Ni-Cr-Mo-V high strength steel at different hydrostatic pressures and pre-stresses
Fig.5  Pitting morphologies of Ni-Cr-Mo-V high strength steel after 168 h immersion in simulated deep-sea environment (5 ℃, 3.5%NaCl) at different hydrostatic pressures and pre-stresses (The pre-stress in the horizontal direction of the plane) (a) macro-pits at 8 MPa and 30%σ0.2 (b) micro-pits at 8 MPa and 60%σ0.2 (c) macro-pits at 8 MPa and 90%σ0.2 (d) micro-pits at 12 MPa and 60%σ0.2 (e) macro-pits at 20 MPa and 90%σ0.2 (f) micro-pits at 28 MPa and 60%σ0.2 (g) morphology at 28 MPa and 90% σ0.2 (h) micro-pits at 28 MPa and 90%σ0.2
Fig.6  Pit sizes at different hydrostatic pressures and pre-stresses(a) 12 MPa and 10%σ0.2(b) 28 MPa and 10%σ0.2(c) 28 MPa and 60%σ0.2
Fig.7  Cumulative probabilities (PC) of pit sizes of Ni-Cr-Mo-V high strength steel at different hydrostatic pressures and pre-stresses(a) 12 MPa and 10%σ0.2(b) 28 MPa and 10%σ0.2(c) 28 MPa and 60%σ0.2
Fig.8  Stress distributions in and around pits at various hydrostatic pressures and pre-stresses (The pre-stress direction is along x axis)

(a) pit at 28 MPa (b) quarter pit at 28 MPa

(c) pit at 28 MPa and 60% s0.2 (d) quarter pit at 28 MPa and 60% s0.2

(e) pit at 28 MPa and 10% s0.2 (f) quarter pit at 28 MPa and 10% s0.2

(g) pit at 12 MPa and 10% s0.2 (h) quarter pit at 12 MPa and 10% s0.2

Fig.9  Stress distributions around adjacent pits aligned along the pre-stress direction (a) and vertical to pre-stress direction (b) (The pre-stress direction is along x axis)
Fig.10  Pitting geometry of Ni-Cr-Mo-V high strength steel at different hydrostatic pressures and pre-stresses (W—diameter of pit, h—depth of pit)
[1] Traverso P, Canepa E.Ocean Eng, 2014; 87: 10
[2] Cao P, Zhou T T, Bai X Q, Yuan C Q.J Chin Soc Corros Prot, 2015; 35: 12
[2] (曹攀, 周婷婷, 白秀琴, 袁成清. 中国腐蚀与防护学报, 2015; 35: 12)
[3] Guo W M, Li W J, Chen G Z.Equip Environ Eng, 2006; 3(1): 10
[3] (郭为民, 李文军, 陈光章. 装备环境工程, 2006; 3(1): 10)
[4] Liu J, Li X B, Wang J.Acta Metall Sin, 2011; 47: 697
[4] (刘杰, 李相波, 王佳. 金属学报, 2011; 47: 697)
[5] Beccaria A M, Poggi G, Arfelli M, Mattogno G.Corros Sci, 1993; 34: 989
[6] Beccaria A M, Poggi G, Gingaud D, Castello P.British Corros J, 1994; 29: 65
[7] Yang Y G, Zhang T, Shao Y W, Meng G Z, Wang F H.Corros Sci, 2010; 52: 2697
[8] Yang Y G, Zhang T, Shao Y W, Meng G Z, Wang F H.Corros Sci, 2013; 73: 250
[9] Liu B, Zhang T, Shao Y W, Meng G Z, Liu J T, Wang F H.Int J Electrochem Sci, 2012; 7: 1864
[10] Paredes-Dugarte S Y, Hidalgo-Prada B.Procedia Mater Sci, 2015; 8: 82
[11] Cruz J L D L, Lindelauf R H A, Koene L, Gutiérrez M A.Electrochem Commun, 2007; 9: 325
[12] Guan L, Zhang B, Yong X P, Wang J Q, Han E H, Ke W.Corros Sci, 2015; 93: 80
[13] Cerit M, Genel K, Eksi S.Eng Fail Anal, 2009; 16: 2467
[14] Beccaria A M, Poggi G.British Corros J, 1985; 20: 183
[15] Zhou J L, Li X G, Chen X Q, Dong C F, Du C W, Lu L.Corros Sci Prot Technol, 2010; 22: 47
[15] (周建龙, 李晓刚, 程学群, 董超芳, 杜翠薇, 卢琳. 腐蚀科学与防护技术, 2010; 22: 47)
[16] Bhandari J, Khan F, Abbassi R, Garaniya V, Ojeda R.J Loss Preven Proc Ind, 2015; 37: 39
[17] Zheng S Q, Li C Y, Qi Y M, Chen L Q, Chen C F.Corros Sci, 2013; 67: 20
[18] Zheng S J, Wang Y J, Zhang B, Zhu Y L, Liu C, Hu P, Ma X L.Acta Mater, 2010; 58: 5070
[19] Beccaria A M, Poggi G, Castello G.British Corros J, 1995; 30: 283
[20] Sun H J, Liu L, Li Y.J Electrochem, 2013; 19: 418
[20] (孙海静, 刘莉, 李瑛. 电化学, 2013; 19: 418)
[21] Pidaparti R M, Patel R R.Mater Lett, 2008; 62: 4497
[22] Li J F, Chen W J, Zhao X S, Ren W D, Zheng Z Q.Trans Nonferrous Met Soc China, 2006; 16: 1171
[23] Hu J P, Liu Z Y, Hu S S, Li X G, Du C W.Surf Technol, 2015; 44(3): 9
[23] (胡建朋, 刘智勇, 胡山山, 李晓刚, 杜翠薇. 表面技术, 2015; 44(3): 9)
[24] Tian W M, Du N, Li S M, Chen S B, Wu Q Y.Corros Sci, 2014; 85: 372
[25] Cerit M.Corros Sci, 2013; 67: 225
[1] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[2] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[3] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[4] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[5] JIN Xinyan, CHU Shuangjie, PENG Jun, HU Guangkui. Effect of Dew Point on Selective Oxidation and Decarburization of 0.2%C-1.5%Si-2.5%Mn High Strength Steel Sheet During Continuous Annealing[J]. 金属学报, 2023, 59(10): 1324-1334.
[6] HOU Xuru, ZHAO Lin, REN Shubin, PENG Yun, MA Chengyong, TIAN Zhiling. Effect of Heat Input on Microstructure and Mechanical Properties of Marine High Strength Steel Fabricated by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(10): 1311-1323.
[7] SUN Yangting, LI Yiwei, WU Wenbo, JIANG Yiming, LI Jin. Effect of Inclusions on Pitting Corrosion of C70S6 Non-Quenched and Tempered Steel Doped with Ca and Mg[J]. 金属学报, 2022, 58(7): 895-904.
[8] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[9] SHI Zengmin, LIANG Jingyu, LI Jian, WANG Maoqiu, FANG Zifan. In Situ Analysis of Plastic Deformation of Lath Martensite During Tensile Process[J]. 金属学报, 2021, 57(5): 595-604.
[10] LV Chenxi, SUN Yangting, CHEN Bin, JIANG Yiming, LI Jin. Influence of Potentionstatic Pulse Technique on Pitting Behavior and Pitting Resistance of 317L Stainless Steel[J]. 金属学报, 2021, 57(12): 1607-1613.
[11] LU Bin, CHEN Furong, ZHI Jianguo, GENG Ruming. Enhanced Welding Properties of High Strength Steel via Rare Earth Oxide Metallurgy Technology[J]. 金属学报, 2020, 56(9): 1206-1216.
[12] LUO Haiwen,SHEN Guohui. Progress and Perspective of Ultra-High Strength Steels Having High Toughness[J]. 金属学报, 2020, 56(4): 494-512.
[13] WANG Li,DONG Chaofang,ZHANG Dawei,SUN Xiaoguang,Chowwanonthapunya Thee,MAN Cheng,XIAO Kui,LI Xiaogang. Effect of Alloying Elements on Initial Corrosion Behavior of Aluminum Alloy in Bangkok, Thailand[J]. 金属学报, 2020, 56(1): 119-128.
[14] Rongyao MA,Changgang WANG,Xin MU,Xin WEI,Lin ZHAO,Junhua DONG,Wei KE. Influence of Hydrostatic Pressure on Corrosion Behavior of Ultrapure Fe[J]. 金属学报, 2019, 55(7): 859-874.
[15] Kaiqiang LI, Lujia YANG, Yunze XU, Xiaona WANG, Yi HUANG. Influence of SO42- on the Corrosion Behavior of Q235B Steel Bar in Simulated Pore Solution[J]. 金属学报, 2019, 55(4): 457-468.
No Suggested Reading articles found!