| [1]Bewlay B P, Jackson M R, Zhao J C, Subramanian P R, Mendirstta M G, Lewandowski J J. MRS Bull, 2003; 28: 646
[2]Bewlay B P, Jackson M R, Zhao J C, Subramanian P R.Metall Mater Trans, 2003; 34A: 2043
[3]Kang Y W, Qu S Y , Song J X , Han Y F. Acta Metall Sin, 2008; 44: 593
(康永旺, 曲士昱, 宋尽霞, 韩雅芳. 金属学报, 2008; 44: 593)
[4]Kim W Y, Tanaka H, Kasama A, Hanada S.Intermetallics, 2001; 9: 827
[5]Guo X P, Guo H S, Yao C F. Int J Mod Phys, 2009;23B: 1093
[6]Qu S Y, Han Y F, Song L G. Intermetallics, 2007;15: 810
[7]Li Z, Peng L M. Acta Mater, 2007; 55: 6573
[8]Guo H S, Guo X P. Scr Mater, 2011; 64: 637
[9]Yang Y, Bewlay B P, Chang Y A. J Phase Equilib Diffus, 2007; 28: 107
[10]Yao C F, Guo X P, Guo H S. Acta Metall Sin, 2008;44: 579
(姚成方, 郭喜平, 郭海生. 金属学报, 2008; 44: 579)
[11]Guo X P, Gao L M. J Aeronaut Mater, 2006; 26(3):47
(郭喜平, 高丽梅. 航空材料学报, 2006; 26(3): 47)
[12]Tian Y X, Guo J T, Cheng G M, Sheng L Y, Zhou L Z, He L L,Ye H Q. Mater Des, 2009; 30: 2274
[13]Cheng G M, He L L. Intermetallics, 2011; 19: 196
[14]Su L F, Jia L N, Feng Y B, Zhang H R, Yuan S N, Zhang H.Mater Sci Eng, 2013; 560: 672
[15]Wang Y, Guo X P. Acta Metall Sin, 2010; 46: 506
(王勇, 郭喜平. 金属学报, 2010; 46: 506)
[16]He Y S, Guo X P. Acta Metall Sin, 2009; 45: 1035
(何永胜, 郭喜平. 金属学报, 2009; 45: 1035)
[17]Zelenitsas K, Tsakiropoulos P. Intermetallics,2005; 13: 1079
[18]Qu S Y, Han Y F, Kang Y W. Sci China, 2009; 52E:37
[19]Sun Z P, Guo X P, He Y S, Guo J M, Yang Y, Chang Y A.Intermetallics, 2010; 18: 997
[20]Geng J, Tsakiropoulos P, Shao G S. Intermetallics,2007; 15: 69
[21]Wang L G, Jia L N, Cui R J, Zheng L J, Zhang H.Chin J Aeronaut, 2012; 25: 292
[22]Fu H Z, Guo J J, Liu L, Li J S. DirectionalSolidification and Processing of Advanced Materials. Beijing:Science Press, 2008: 29
(傅恒志, 郭景杰, 刘林, 李金山. 先进材料定向凝固. 北京:科学出版社, 2008: 29)
[23]Zhou Y H, Hu Z Q, Jie W Q. Solidification Processing. Beijing: China Machine Press, 1998: 158
(周尧和, 胡壮麒, 介万奇. 凝固技术. 北京: 机械工业出版社, 1998:158)
[24]Hu H Q. Fundamental of Metallic Solidification. 2nd Ed., Beijing: China Machine Press, 2000: 165
(胡汉起. 金属凝固原理. 第2版, 北京: 机械工业出版社, 2000: 165)
[25]Tang L, Ma C L, Zhao X Q. Rare Met Mater Eng,2009; 38: 8 |