| FIRST-PRINCIPLES STUDY OF STACKING FAULT ENERGY AND DEFORMATION TWIN\par ENERGY IN Al-Mg ALLOYS |
| DONG Minghui, HAN Peide, ZHANG Caili, YANG Yanqing, ZHANG Lili, LI Hongfei |
1) College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024
2) Key Laboratory of Interface Science and Engineering in Advanced Materials of Taiyuai University of Technology, Ministry of Education, Taiyuan 030024 |
|
Cite this article:
DONG Minghui HAN Peide ZHANG Caili YANG Yanqing ZHANG Lili LI Hongfei. FIRST-PRINCIPLES STUDY OF STACKING FAULT ENERGY AND DEFORMATION TWIN\par ENERGY IN Al-Mg ALLOYS. Acta Metall Sin, 2011, 47(5): 573-577.
|
|
|
Abstract By using first--principles method based on the density functional theory (DFT), the stacking fault energy (SFE) and deformation twin energy (DTE) for the (111)[112] slip system of pure Al metal and Al-Mg alloys were investigated. The dependence of these SFE and DTE on solid--solution Mg content and its accupation were specifically analyzed. Two major approximations were made in the process of calculation, which were local density approximation (LDA) and generalized gradient approximation (GGA-PW91), respectively. The calculated SFE values by using GGA-PW91 exhibit an excellent agreement with corresponding experimental measurements. For pure Al metal, the calculated SFE values are greater than those of DTE. Moreover, it is found that under the same deformation conditions, the DTE in pure Al and Al-Mg alloys increase monotonically with the increase of deformation twin thickness. In addition, the calculated results shows that 6-layer twin possesses the lowest DTE, which is probably due to its mirror symmetry structure. Also noteworthy, our calculations reveal a noticeable decreased tendency of SFE and DTE with Mg content increasing, while Mg occupying on stacking fault and twin boundary most likely increases SFE and DTE. There are no considerably detected effects of Mg atomic occupancy variation in Al-Mg alloy on its cohesive energy and formation energy.
|
|
Received: 15 October 2010
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.50874079 and 51002102), Taiyuan Science and Technology Project (No.100115105) and Education Department of Shanxi Province (No.20080010) |
| [1] Fanourgakis G S, Pontikis V, Zerah G. Phys Rev, 2003; 67B: 094102[2] Gang L, Kioussis N, Bulatov V V, Kaxiras E. Phys Rev, 2000; 62B: 3099[3] Rester M, Motz C, Pippan R. Scr Mater, 2008; 58: 187[4] Zhu Y T, Narayan J, Hirth J P, Mahajan S, Wu X L, Liao X Z. Acta Mater, 2009; 57: 3763[5] Zhao Y H, Zhu Y T, Liao X Z, Horita Z, Langdon T G. Appl Phys Lett, 2006; 89: 121906[6] Yamakov V, Wolf D, Phillpot S R. Acta Mater, 2002; 50: 5005[7] Hai S, Tadmor E B. Acta Mater, 2003; 51: 117[8] Chen M W, Ma E, Hemker K J, Sheng H W, Wang Y M, Cheng X M. Science, 2003; 300: 1275[9] Liu M, Roven H J, Murashkin M, Valiev R Z. Mater Sci Forum, 2008; 579: 147[10] Zhang J M, Xie L J, Xu K W. Acta Metall Sin, 2007; 43: 182(张建民, 解丽娟, 徐可为. 金属学报, 2007; 43: 182)[11] Wu X Z, Wang R, Wang S F, Wei Q Y. Appl Surf Sci, 2010; 256: 6345[12] Wu J, Wen L, Tang B Y, Peng L M, Ding W J. Solid State Sci, 2011; 13: 120[13] Heino P, Perondi L, Kaski K, Ristolainen E. Phys Rev, 1999; 60B: 14625[14] Schulthess T C, Turchi P E A, Gonis A, Nieh T G. Acta Mater, 1998; 46: 2215[15] Kohn W, Sham L. Phys Rev, 1965; 140: A1133[16] Milman V, Winkler B, White J A, Pickard C J, Payne M C, Akhmatskaya E V, Nobes R H. Int J Quant Chem, 2000; 77: 895[17] Segall M D, Lindan P J D, Probert M J, Pickard C J, Hasnip P J, Clark S J, Payne M C. J Phys, 2002; 14: 2717[18] Mattsson A E, Schultz P A, Desjarlais M P, Mattsson T R, Leung K. Model Simul Mater Sci Eng, 2005; 13: R1[19] Payne M C, Teter M P, Allan D C, Arials T A, Joannopoulos J D. Rev Mod Phys, 1992; 64: 1045[20] Perdew J P, Chevary J A, Vosko S H, Jackson K A, Perderson M R, Singh D J, Fiolhais C. Phys Rev, 1992; 46B: 6671[21] Meyer R, Lewis L J. Phys Rev, 2002; 66B: 052106[22] Hirth J P, Lothe J. Theory of Dislocations. 2nd Ed., New York: Wiley, 1982: 839[23] Baskes M I. Phys Rev, 1992; 46B: 2727[24] Ogata S, Li J, Yip S. Science, 2002; 298: 807[25] Hartford J, Von Sydow B, Wahnstr¨om G, Lundqvist B I. Phys Rev, 1998; 58B: 2487[26] Wang Y F, Zhang W B, Wang Z Z, Deng Y H, Yu N, Tang B Y, Zeng X Q, Ding W J. Comput Mater Sci, 2007; 41: 78[27] Zhang C L, Han P D, Yan X, Wang C, Xia L Q, Xu B S. J Phys, 2009; 42D: 125403[28] Mola R, Dziado´n A. Arch Foundry Eng, 2008; 8: 127 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|