| ORTHORHOMBIC PHASE TRANSFORMATIONS IN TITANIUM ALLOYS AND THEIR APPLICATIONS |
| YANG Rui, HAO Yulin, Obbard E G, DONG Limin, LU Bin |
|
Cite this article:
YANG Rui HAO Yulin Obbard E G DONG Limin LU Bin. ORTHORHOMBIC PHASE TRANSFORMATIONS IN TITANIUM ALLOYS AND THEIR APPLICATIONS. Acta Metall Sin, 2010, 46(11): 1443-1449.
|
|
|
Abstract The link and difference between orthorhombic phase transformations in β-type titanium alloys and in Ti3Al containing high concentrations of transition metal elements such as Nb are first outlined in this paper. Recent investigations on these transformations conducted in the authors' group are reviewed followed by discussions of remaining problems. Three examples were presented to illustrate the applications of the orthorhombic phase transformations: design and development of superelastic titanium alloys for biomedical use, preparation of ultra-fine basketweave microstructure of titanium alloy wire for fastener manufacturing, and sheet and foil production of alloys based on Ti2AlNb.
|
|
Received: 17 September 2010
|
| [1] Shih C H, Averbach B L, Cohen M. Trans AIME, 1955; 203: 183
[2] Bagariatskii Y A, Nosova G I, Tagunova T V. Dok Akad Nauk SSSR, 1958; 122: 593
[3] Jepson K S, Brown A R G, Gray J A. In: Jaffee R I, Promisel N E, eds., The Science, Technology and Application of Titanium (Proc 1st Int Conf Titanium), London: Pergamon, 1970: 677
[4] Williams J C. In: Jaffee R I, Burte H M, eds., Titanium Science and Technology (Proc 2nd Int Conf Titanium), New York: Plenum, 1973: 1433
[5] Flower H M, Davis R,West D R F. In: Williams J C, Belov A F, eds., Titanium and Titanium Alloys: Scientific and Technological Aspects (Proc 3rd Int Conf Titanium), New York: Plenum, 1982: 1703
[6] Banerjee D, Gogia A K, Nandy T K, Joshi V A. Acta Metall, 1988; 36: 871
[7] Hao Y L, Li S J, Sun S Y, Zheng C Y, Hu Q M, Yang R. Appl Phys Lett, 2005; 87: 091906
[8] Hao Y L, Li S J, Sun B B, Sui M L, Yang R. Phys Rev Lett, 2007; 98: 216405
[9] Cui J P, Hao Y L, Li S J, Sui M L, Li D X, Yang R. Phys Rev Lett, 2009; 102: 045503
[10] Li S J, Cui T C, Hao Y L, Yang R. Acta Biomater, 2008; 4: 305
[11] Bendersky L A, Roytburd A, Boettinger W J. Acta Metall Mater, 1994; 42: 2323
[12] Obbard E G, Hao Y L, Akahori T, Talling R J, Niinomi M, Dye D, Yang R. Acta Mater, 2010; 58: 3557
[13] Obbard E G. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2010
[14] Obbard E G, Hao Y L, Talling R J, Li S J, Zhang Y W, Dye D, Yang R. Acta Mater, in press
[15] Gao X, Huang M, Brinson L C. Int J Plast, 2000; 16: 1345
[16] Heinen R, Hackl K, Windl W, Wagner M F. Acta Mater, 2009; 57: 3856
[17] Afonso C R, Ferrandini P L, Ramirez A J, Caram R. Acta Biomater, 2010; 6: 1625
[18] Hao Y L, Li S J, Sun S Y, Yang R. Mater Sci Eng, 2006; A441: 112
[19] Petry W, Heiming A, Trampenau J. Alba M, Herzig C, Schober H R, Vogl G. Phys Rev, 1991; 43B: 10933
[20] Li S J, Yang R, Niinomi M, Hao Y L, Cui Y Y, Guo Z X. Mater Sci Technol, 2005; 21: 678
[21] Hu Q M, Yang R, Xu D S, Hao Y L, Li D. Phys Rev, 2003; 68B: 054102 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|