| EFFECT OF APPLIED POTENTIAL ON SCC OF X80 PIPELINE STEEL AND ITS WELD JOINT IN KU’ERLE SOIL SIMULATED SOLUTION |
| CHEN Xu, WU Ming, HE Chuan, XIAO Jun |
| College of Petroleum Engineering, Liaoning Shihua University, Fushun 113001 |
|
Cite this article:
CHEN Xu WU Ming HE Chuan XIAO Jun. EFFECT OF APPLIED POTENTIAL ON SCC OF X80 PIPELINE STEEL AND ITS WELD JOINT IN KU’ERLE SOIL SIMULATED SOLUTION. Acta Metall Sin, 2010, 46(8): 951-958.
|
|
|
Abstract Potentiodynamic polarization technique and slow strain rate testing (SSRT) were employed to study the stress corrosion cracking (SCC) behavior of a welded X80 pipeline steel in Ku’erle soil simulated solution. Fracture surfaces were observed by SEM under different applied potential conditions. The results show that the polarization curves of the base metal and weld joint represent the typical characteristics of active dissolution. It is found that cracks are generally initiated at corrosion pits and inclusions under anode polarization and open circuit potential. The crack generation mechanism of X80 pipeline base steel and weld metal are attributed to the dissolution at anode. When the applied potential is −900 mV (vs SCE), the base metal exhibites lower SCC sensitivity due to cathodic protection while under the same condition welded joins higher SCC sensitivity. Both the base metal and weld joins exhibite higher SCC sensitivity under −1200 mV (vs SCE) polarization potential and their cracking generation mechanism is hydrogen induced cracking (HIC) due to the synergistic action of stress and hydrognCommonly the weld joint is more sensitive to SCC than the base etal under the same applid potential, and fractures are usually presented in heat affected zone (HAZ) and this is attributed to metallurgical phase transformation and residual stress enerated during welding process.
|
|
Received: 01 March 2010
|
| Fund: Supported by National Natural Science Foundation of China (No.50771053) |
| [1] Li J, Elboujdaini M, Gao M, Revie R W. Mater. Sci. Eng, A, 2008, 486: 496
[2] Liu Z Y, Li X G, Zhang Y R, Du C W. Acta Metall Sin (English Letters), 2009, 22: 58
[3] Li M C, Cheng Y F. Electrochimica Acta, 2007, 52: 8111
[4] Fazzini P G, Otegui J L. International Journal of Pressure Vessels and Piping, 2007, 84: 739
[5] Liu Z Y, Li X G, Du C W, Cheng Y F. Corros. Sci., 2009, 51: 2863
[6] Gamboa E, Linton V, Law M. Int. J. Fatigue, 2008, 30: 850
[7] Wang J Q, Atrens A. Corros. Sci., 2003, 45: 2199
[8] Krist K., Leewis L., Willmoff M. Pipeline & Gas Journal, 1998, 225: 49
[9] Parkins R N, Zhou S. Corr. Sci, 1997, 39: 159
[10] Parkins R N, Zhou S. Corr. Sci, 1997, 39: 175
[11] Danielson Mike J, Jones Russell H, Krist Kevin. CORROSION/2000, NACE International, Houston, TX, 2000, Paper No.359
[12] Charles E A, Parkins R N. Corrosion, 1995, 51: 518
[13] Pikey A K, Lambert S B, Plumtree A. Corrosion, 1995, 51: 91
[14 ]Wang J Q, Atrens A, Cousens D R, et al. Journal of Materials Science, 1999, 34:1711
[15] Mao X, Liu X, Revie R W. Corrosion, 1994, 50: 651
[16] :Cao C N. Corrosion of Metals in Nature Environment in China. Beijing: Chemical Industry Press, 2004: 286
(曹楚南. 中国材料的自然环境腐蚀. 北京: 化学工业出版社, 2004: 286 )
[17] Van Boven G, Chen W, Rogge R. Acta Mater, 2007, 55: 29
[18] Chu R, Chen W, Wang S H, et al. Corrosion, 2004, 60: 275
[19] Davies D H, Burstein G T. Corrosion, 1980, 36: 416
[20] Li M C, Cheng Y F. Electrochimica Acta, 2008, 53: 2831
[21] Zhang T ,Sun X L ,Chen J S ,et al. Pipeline Technique and Equipment , 2004, 2:33
(张涛,孙新岭,陈居术,等.氢在高强度管道钢应力腐蚀中的作用[J].管道技术与设备,2004, 2:33)
[22] Zhang G A, Cheng Y F. Electrochimica Acta, 2009, 55: 316
[23] Zhang G A, Cheng Y F. Corr. Sci, 2009, 51: 1714
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|