| EFFECT OF COOLING RATE ON MICROSTRUCTURE OF DEFORMED AND UNDEFORMED X80 PIPELINE STEELS |
| DENG Wei, GAO Xiuhua, QIN Xiaomei, GAO Xin, ZHAO Dewen, DU Linxiu |
| State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819 |
|
Cite this article:
DENG Wei GAO Xiuhua QIN Xiaomei GAO Xin ZHAO Dewen DU Linxiu. EFFECT OF COOLING RATE ON MICROSTRUCTURE OF DEFORMED AND UNDEFORMED X80 PIPELINE STEELS. Acta Metall Sin, 2010, 46(8): 959-966.
|
|
|
Abstract The effects of cooling rate and deformation on microstructures of an X80 pipeline steel were investigated by thermo–mechanically simulated tests heated up to the same temperature and cooled at different rates under 0 and 0.7 true strain deformation. The results reveal that the start temperature for bainite transformation will be increased by 30—80 ℃higher under 0.7 true strain than under no deformation. But the increase of cooling rate depresses the start temperature for bainite transformation and accelerates the progress of its transformation. It is found that the microstructure of the cooled samples without deformation is all composed of bainite with prior austenite grain boundaries (PAGB), but it is complicated for the cooled samples under 0.7 true strain. In the range of 1—40 ℃/s, with the increase of cooling rate, microstructures appeare successively such as polygonal ferrite, quasi–polygonal ferrite, massive ferrite, granular bainite, acicular ferrite (+ granular bainite) and athy bainite. Full martnsite steel can be acheved by quenching. Under current experiment conditions, acicular ferrite can be obtained n the steel at cooling rates of 10—20 ℃/s. In this cooing ate range, the fraction of high angle grain boundaries (HAGBs) inceases and the grain size decreases with the increase of cooling rate.
|
|
Received: 05 January 2010
|
| Fund: Supported by the Fundamental Research Funds for the Central Universities (No.N090607002), National Natural Science Foundation of China (No.50474015) and State Key Laboratory Self–determination Foundation (No.RAL–SD–2008–2) |
| [1] Kim Y M, Kim S K, Lim Y J, Kim N J. ISIJ Int, 2002; 42: 1571
[2] Zhao M C, Shan Y Y, Xiao F R, Yang K, Li Y H. Mater Lett, 2002; 57: 141
[3] Bakkaloglu A. Mater Lett, 2002; 56: 200
[4] Zhao M C, Yang K, Shan Y Y. Mater Lett, 2003;57: 1496
[5] Zhao M C, Yang K, Xiao F R, Shan Y Y. Mater Sci Eng A,2003;355: 126
[6] Xiao F R, Liao B, Ren D L, Shan Y Y, Yang K. Mater Charact, 2005;54: 305
[7] Kim Y M, Lee H, Kim N J. Mater Sci Eng A, 2008;478: 361
[8] Pickering F B. Physical Metallurgy and Design of Steels. Essex: Applied Science Publishers Ltd., 1978: 64
[9] Dutta B, Valde′s E, Sellars C M. Acta Metall., 1992; 40 (4): 653
[10] Saito Y, Kimura M, Tanaska M, Sekine T, Tsubota K, Tanaka T. Kawasaki Steel Technical Report. 1984; 3: 12
[11] Aaronson H I, Enomoto M, Furuhara T, Reynolds W T. In: I. Tamura eds., Thermec 88, Int. Conf. on Physical Metallurgy of Thermomechanical Processing of Steels and Other Metals, Tokyo: Iron and Steel Institute of Japan. 1988; 1: 80
[12] Cotrina E, Iza-Mendia A, López , Gutiérrez I. Metall Mater Trans, 2004; A 35(1): 93
[13] Umemoto M, Guo Z H, Tamura I. Mater Sci Technol, 1987; 3: 249
[14] Honeycombe R W K. Steels Microstructures and Properties. London: Edward Arnold Pub. Ltd., 1980: 43
[15] Zhong Y, Xiao F R, Zhang J W. Acta Materialia, 2006; 54: 435
[16] Bhadeshia H K D H. Mater Sci Eng A, 1999; 273-275: 58
[17] Manabu T. Current Opinion in Solid State Mater Sci, 2004; 8: 213
[18] Liu Sh K, Yang L, Zhang J, Zhu D G. Acta Metall Sin, 1992; 28: A513
(刘世楷, 杨柳, 张筠, 朱德贵. 金属学报, 1992; 12: A513)
[19] Eghbali B, Abdollah-zadeh A. Scr Mater, 2006; 54: 1205
[20] Gregg J M, Bhadeshia H K D H. Metall Mater Trans, 1994; A 25:1603
[21] Quidort D, Bréchet Y. Scr Mater, 2002; 47: 151
[22] Li J, Sun F Y. Acta Metall Sin, 1990; 26: A 396
(李箭, 孙福玉.金属学报, 1990; 26: A396)
[23] Zhang B, Zhang H B. J Shanghai Jiaotong Uni, 2003; 37: 1522
(张斌, 张鸿冰.上海交通大学学报, 2003; 37: 1522)
[24] Bai D Q, Yue S, Maccagno T M, Jonas J J. Metall Mater Trans, 1998; A 29: 989
[25] Chang L C. Mater Sci Eng A, 2004; 368: 175
[26] Quidort D, Bréchet Y. ISIJ Int, 2002; 42: 1010
[27] Zhao J Z, Mesplont C , De Cooman B C. ISIJ Int, 2001; 41: 492
[28] Xu Z Y, Liu S K. Bainite Transformation and Bainite. Beijing: Science Press, 1991; 6: 179
(徐祖耀,刘世楷.贝氏体相变与贝氏体. 北京: 科学出版社,1991; 6: 179)
[29] Zhang W, Wu X C, Min Y A. Trans Mater Heat Treat, 2008; 29: 78
(张伟, 吴晓春, 闵永安. 材料热处理学报, 2008; 29: 78)
[30] Liu Z C, Ren H P. Diffusion Phase Transformation of Supercooled Austenite. Beijing: Science Press, 2007; 12: 88
(刘宗昌, 任慧平. 过冷奥氏体扩散型相变. 北京: 科学出版社, 2007; 12: 88)
[31] Cizek P, Wynne B P, Davies C H J, Muddle B C, Hodgson P D. Metall Mater Trans, 2002; A 33: 1331
[32] Hanzaki A Z, Pandi R, Hodgson P D, Yue S. Metall Mater Trans, 1993; A 24: 2657
[33] BAl D Q. S. Yue S, Maccagno T M, Jonas J J. ISIJ Int. 1998; 38: 371
[34] Bengochea R, Lo′Pez B, Gutierrez I. Metall Mater Trans, 1998; A 29: 417
[35] Fang H S. Bainite Transformation. Beijing: Science Press, 1999; 2: 59
(方鸿生. 贝氏体相变. 北京: 科学出版社, 1999; 2: 59)
[36] Bramfitt B L, Speer J G.. Metall Mater Trans, 1990; A 21: 817
[37] Yang Z G, Fang H S. Current Opinion in Solid State and Materials Science, 2005; 9: 277
[38] Singh S B, Bhadeshia H K D H. Mater Sci Eng, 1998; A245: 72
[39] Hwang B, Kim Y G, Lee S. Metall Mater Trans, 2005; 36A: 2107
[40] Díaz-Fuentes M, Madariga I, Gutiérrez I. Mater Sci Forum, 1998; 284–286: 245
[41] Rodríguez-Ibabe J M. Mater Sci Forum, 1998; 284–286: 51
[42] Diza-Fuentes M, Iza-Mendia A, Gutierrez I. Metall Mater Trans A, 2003; 34A: 2505
[43] Gourgues A F, Flower H M, Lindley T C. Mater Sci Technol, 2000; 16: 26
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|