Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (1): 34-40    DOI:
Current Issue | Archive | Adv Search |
HIGH TEMPERATURE CORROSION-EROSION BEHAVIOR OF Cr-BEARING STEELS
A. V. LEVY Institute of Metal Research; Academia Sinica. Shenyang; Lawrence Berkely Lab.; University of California; USAMAN Yongfa Associate Professor;Istitute of Metal research;Academia Sintea;shenyang
Cite this article: 

A. V. LEVY Institute of Metal Research; Academia Sinica. Shenyang; Lawrence Berkely Lab.; University of California; USAMAN Yongfa Associate Professor;Istitute of Metal research;Academia Sintea;shenyang. HIGH TEMPERATURE CORROSION-EROSION BEHAVIOR OF Cr-BEARING STEELS. Acta Metall Sin, 1988, 24(1): 34-40.

Download:  PDF(2074KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Combined corrosion-erosion (C-E) behavior of some commercial steelscontaining 2.25--25 wt-%Cr have been investigated at 850℃ using air as carryinggas and 130μm dia. SiC or Al_2O_3 as erodents. It was found that C-E behaviorstrongly depends on the corrosion resistance of steels. The C-E resistance increaseswith increasing Cr content, and a drastic raise of the resistance occurs at about9 wt-%Cr. Obvious influences of the nature and shape of the particles on the C-Erate of steels was noticed. Mechanisms of material degradation have also beendiscussed.
Key words:  Cr-Bearing steel      erosion     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/34

1 Maasberg J A, Levy A V. Wear, 1981; 73: 355
2 Nagarajan Y, Wright I G. In: Rapp R A ed., High Temperature Corrosion, NACE, 1983: 398--405
3 Hill V L, Verely E J Jr. In: Proceedings of Corrosion Erosion Behavior of Materials, St Lours USA 1978: 695
4 Tabakoff W, Vittal B V R. Wear, 1983; 86: 89
5 Wright I G, Nagarajan V. In: Proceedings of Corrosion Erosion Behavior of Materjals. St Lours USA, 1978: 269
6 Ives L K, Ruff A W. In: Adler W F ed., Erosion: Frevention and Useful Application, ASTM STP 664, ASTM, 1979: 5
7 Hutchings I. In: Adler W F ed., Frosion: Prevention and Useful Application, ASTM STP--664, ASTM, 1979: 59
8 Khanna A S, Jha B B, Kaj B. Oxid Met, 1985 23: 159
9 Kuroda K, Labun P A. Welsch G, Mitchell T E. Oxid Met, 1983: 19: 117
10 Levy A V, Man Y F. Wear, 1986; 111: 135
11 Levy A V, Man Y F. NACE Corrosion 85, paper №338, Boston MA 1985
[1] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[2] ZHANG Shihong, HU Kai, LIU Xia, YANG Yang. Corrosion-Erosion Mechanism and Research Prospect of Bare Materials and Protective Coatings for Power Generation Boiler[J]. 金属学报, 2022, 58(3): 272-294.
[3] MA Minjing, QU Yinhu, WANG Zhe, WANG Jun, DU Dan. Dynamics Evolution and Mechanical Properties of the Erosion Process of Ag-CuO Contact Materials[J]. 金属学报, 2022, 58(10): 1305-1315.
[4] LIU Haixia, CHEN Jinhao, CHEN Jie, LIU Guanglei. Characteristics of Waterjet Cavitation Erosion of 304 Stainless Steel After Corrosion in NaCl Solution[J]. 金属学报, 2020, 56(10): 1377-1385.
[5] Jianxiang DING,Wubian TIAN,Dandan WANG,Peigen ZHANG,Jian CHEN,Zhengming SUN. Arc Erosion and Degradation Mechanism ofAg/Ti2AlC Composite[J]. 金属学报, 2019, 55(5): 627-637.
[6] Yanxin QIAO,Shuo WANG,Bin Liu,Yugui ZHENG,Huabing LI,Zhouhua JIANG. SYNERGISTIC EFFECT OF CORROSION AND CAVITATION EROSION OF HIGH NITROGEN STAINLESS STEEL[J]. 金属学报, 2016, 52(2): 233-240.
[7] FU Chong, WANG Junbo, YANG Minge, HOU Jinli, DING Bingjun. MICROSTRUCTURE AND ELECTRICAL PROPERTIES OF Ag/(Sn0.8La0.2)O2 COATING PREPARED BY PLASMA SPRAYING[J]. 金属学报, 2013, 49(3): 325-329.
[8] FANG Xinxian BAI Yunqiang WANG Zhangzhong. EROSION CORROSION BEHAVIOUR OF J4 STAINLESS STEEL AND ELECTROLESS PLATING COATINGS OF Ni–P AND Ni–Cu–P IN LIQUID–SOLID TWO–PHASE FLOW[J]. 金属学报, 2010, 46(2): 239-244.
[9] LIU Shihan CHEN Darong. MECHANICS MECHANISM OF DUPLEX STEEL CAVITATION DAMAGE[J]. 金属学报, 2009, 45(5): 519-526.
[10] . [J]. 金属学报, 2007, 43(6): 648-652 .
[11] ZHANG Anfeng; WANG Yuyue; XING Ji; ong; LI Changjiu. SYNERGISTIC EFFECTS BETWEEN EROSION AND CORROSION OF TWO COATINGS AND TWO STEELS IN TWO--PHASE FLOW[J]. 金属学报, 2004, 40(4): 411-415 .
[12] JIANG Shengli; ZHENG Yugui; YAO Zhiming. Damage Behavior of 20SiMn Low Alloy Steel in Slurry with Different Particle Sizes[J]. 金属学报, 2004, 40(2): 163-167 .
[13] YE Wujun;FENG Di;CHEN Beijing;LUO Heli (Central Iron and Steel Research institute; BeiJing 100081). EFFECT OF METALLURGICAL FACTORS ON THE RESISTANCE OF CAVITATION EROSION OF Ni_3Al BASED ALLOYS[J]. 金属学报, 1998, 34(11): 1163-1166.
[14] WEI Xiangyun;ZHENG Yugui;ZHANG Yusheng;YAO Zhiming;ZHANG Yadong;ZHANG Shaopeng; KE Wei(Corrosion Science Laboratory;Institute of Corrosion and Protection of Metals; The Chinese Academy;of Sciences;Shenyang). EFFECT OF MICROSTRUCTURE AND ELEMENT DISTRIBUTION ON EROSION-CORROSION BEHAVIOUR OF AN IRON BASE CAST ALLOY[J]. 金属学报, 1994, 30(2): 91-96.
[15] ZHENG Qiguang;LI Jiarong;LI Zaiguang Huazhohg University of Science and Technology; Wuhan; HU Weiguang PLA Unit No. 38609; TIAN Hongye PLA Factory No. 4808. EFFECT OF LASER TREATMENT ON CAVITATION EROSION RESISTANCE OF DIESEL CYLINDER[J]. 金属学报, 1991, 27(3): 116-120.
No Suggested Reading articles found!