MORPHOLOGY OF (Mn, Fe)S SINGLE CRYSTAL GROWTH IN CAST STEEL
JIANG Xishan;GONG Yansheng;ZHANG Guichang Research Institute of Qiqihar Steel Plant; Qiqihar Heilongjiang
Cite this article: 

JIANG Xishan;GONG Yansheng;ZHANG Guichang Research Institute of Qiqihar Steel Plant; Qiqihar Heilongjiang. MORPHOLOGY OF (Mn, Fe)S SINGLE CRYSTAL GROWTH IN CAST STEEL. Acta Metall Sin, 1988, 24(4): 295-298.

Download:  PDF(1413KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The step pattern of single crystal growth and the morphology at equilbriiumstate of (Mn, Fe)S on the wall of micro-voids in ZG25 cast steel have been observed using scan-ning electron microscope. The face-centred cubic (Mn, Fe)S single crystal at equilibrium stateis shown to be tetrakaidecahedron consisted of eight {111} planes and six {100} planes, and isa typical example of the O_h-m3m cubic crystal system.
Key words:  cast steel      (Mn      Fe)S      single crystal growth      crystal morphology     
Received:  18 April 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I4/295

1 闵乃本.晶体生长的物理基础,上海科学技术出版社,1982:309,312~
[1] GENG Yaoxiang, TANG Hao, XU Junhua, ZHANG Zhijie, YU Lihua, JU Hongbo, JIANG Le, JIAN Jianglin. Formability and Mechanical Properties of High-Strength Al-(Mn, Mg)-(Sc, Zr) Alloy Produced by Selective Laser Melting[J]. 金属学报, 2022, 58(8): 1044-1054.
[2] Huadong YAN,Hui JIN. Three-Dimensional Characteristics and Morphological Evolution of Micro/Meso Pores inG20Mn5N Steel Castings[J]. 金属学报, 2019, 55(3): 341-348.
[3] Yinhui ZHANG, Qiang FENG. Effects of W on Creep Behaviors of Novel Nb-Bearing Austenitic Heat-Resistant Cast Steels at 1000 ℃[J]. 金属学报, 2017, 53(9): 1025-1037.
[4] Yinhui ZHANG,Mei LI,Larry A GODLEWSKI,Jacob W ZINDEL,Qiang FENG. EFFECTS OF N ON CREEP PROPERTIES OF AUSTENI-TIC HEAT-RESISTANT CAST STEELS DEVELOPEDFOR EXHAUST COMPONENT APPLICATIONSAT 1000 ℃[J]. 金属学报, 2016, 52(6): 661-671.
[5] SU Bin HAN Zhiqiang ZHAO Yongrang SHEN Bingzhen ZHANG Lianzhen LIU Baicheng. CA MODELING OF PHASE TRANSFORMATION IN ASTM A216 WCA CAST STEEL DURING SOLIDIFICATION AND COOLING PROCESS[J]. 金属学报, 2011, 47(11): 1388-1395.
[6] ZHANG Jie WANG Qing WANG Yingmin DONG Chuang. STUDY ON THE CLUSTER--BASED MODEL OF Ni30Cu70 SOLID SOLUTION WITH Fe AND Mn AND ITS CORROSION RESISTANCE[J]. 金属学报, 2009, 45(11): 1390-1395.
[7] LI Defu;LIN Bainian; YAN Yonggui; AN Geying (Harbin Institute of Technology;Harbin 150001)(Manuscript received 1994-08-29; in revised form 1995-02-27). EXPERIMENTAL MODELLING FOR RHEOLOGICAL PROPERTIES OF CAST STEEL[J]. 金属学报, 1995, 31(21): 389-393.
[8] LIN Jialiu;ZHU Shigen;YU Zhenzong Tsinghua University; Beijing. RHEOLOGICAL BEHAVIOUR OF CAST STEEL AT SOLIDIFICATION TEMPERATURE[J]. 金属学报, 1991, 27(5): 110-115.
[9] ZHANG Wei;LI Longsheng;CHENG Ji Dalian University of Technology Dalian University of Technology;Dalian;Liaoning 116023. INFLUENCE OF RARE EARTH ON GRAIN BOUNDARY CRACKING OF CAST STEEL Ni9[J]. 金属学报, 1990, 26(2): 79-82.
[10] XUE Bai;LIU Jun Deportment of Physfcs;University of Science and Technology of China;Hefei;ZHANG Taiyong;ZHENG Zhaobo University of Science and Technology of China; Hefei. GROWTH OF LARGE SINGLE CRYSTAL Cu FOR NEUTRON MONOCHROMATOR USE[J]. 金属学报, 1988, 24(1): 60-62.
No Suggested Reading articles found!