| STRESS RELAXATION BEHAVIOUR OF TITANIUM |
| XIA Yuebo;WANG Zhongguang Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
XIA Yuebo;WANG Zhongguang Institute of Metal Research; Academia Sinica; Shenyang. STRESS RELAXATION BEHAVIOUR OF TITANIUM. Acta Metall Sin, 1989, 25(2): 5-9.
|
|
|
Abstract Stress relaxation study of commercial pure titanium under tensile de-formation shows that the stress relaxation behaviour of it relates to the level ofdeformation. The relaxed stress △σ is independent of amplitude of stress dip in therange of certain deformation, and it is dependent of stress level at beginning ofstress relaxation in determined relaxation time t_R. The back (critical) stress σ_c andflow stress σ_c exhibit same change with the strain. The effective stress at the dislo-cation in materials σ~* increases with increasing strain ranging under low strain, andkeeps constant under higher strain.
|
|
Received: 18 February 1989
|
1 #12 2 Conrad H, Okazaki K. Scr Metall, 1970; 4: 259 3 Bocek M, Schneider H, Sindelar P. Mater Sci Eng, 1971; 8: 161 4 Bocek M, Preininger D, Bressers J. Mater Sci Eng, 1974; 14: 67 5 Yin C, Doener M, Conrad H. Metall Trans, 1975; 6A: 1901 6 Manjoine M J. Pressure Vessel and Piping Technology 1985, Decade of Progress, American Society of Mechanical Engineer, New York, 1985: 521--527 7 Chen P S, Herman W A, Pense A W. WRC Bull, 1985; (302) : 15--22 8 Babichev A P, Sihirskii V V, Shevtson S N. Fiz Khim Mekh Mater, 1985; 21 (1) : 55--59 9 Bengstron J, Ericsson T. Surf Eng, 1986; 2: 115 10 Okazaki K, Aono Y, Kaneyuki T. Mater Sci Eng, 1978; 33 (2) : 253 11 Han Y, Chaturvedi M C. Mater Sci Eng, 1987; 85: 59 12 Guiu F. Philos Mag, 1969; 20 (163) : 51 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|