DRIVING FORCE OF BAINITIC TRANSFORMATION FOR Fe-Mn-C ALLOYS
YANG Liu;FANG Hongsheng;CHEN Nanping Tsinghua University; Beijing
Cite this article: 

YANG Liu;FANG Hongsheng;CHEN Nanping Tsinghua University; Beijing. DRIVING FORCE OF BAINITIC TRANSFORMATION FOR Fe-Mn-C ALLOYS. Acta Metall Sin, 1989, 25(4): 30-35.

Download:  PDF(455KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The regular solution model developed by M. Hillert et al is appliedto calculate the driving force of bainitic transformation for Fe-C-Mn ternary alloysin the intermediate temperature range. Focus is made on the thermodynamical dis-cussions for both diffusional and shear mechanisms for bainitic transformations indifferent temperature ranges.
Key words:  bainite      isothermal transformation      thermodynamics     
Received:  18 April 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I4/30

1 Hsu T Y (Xu Zuyao) (徐祖耀), Mou Yiwen (牟翊文). Acta Metall, 1984; 32: 1469
2 Hillert M, Staffanson L I. Acta Chem Scand, 1970; 24: 3618
3 Sharma R C, Purdy Q R, Kirkaldy J S. Metall Trans, 1979; 10A: 1119
4 Ulhrenius B. In: Doane D V, Kirkaldy J S eds., Hardenability Concepts with Application to Steel, AIME, 1978: 28
5 Hsu T Y (Xu Zuyao) (徐祖耀), Chang Hongbing (张鸿冰), Luo Shoufu. J Mater Sci, 1983; 18: 3206
6 Orr R L, Chipman J. Trans. TMS-AIME, 1967; 239: 630
7 赵宇新,李朋兴,徐祖耀.金属学报,1986; 22: A130
8 Himmelblau D M. Applied Nonlinear Programing, New York: McGrow-Hill, Book Company, 1972
9 杨柳.清华大学工学博士论文,1988
10 Heheman R F. Phase Transformation, Metals Park, Ohio: ASM, 1970: 397
11 Coates D E. Metall Trans, 1973; 4A: 2313
12 Hsu T Y (Xu Zuyao) (徐祖耀), Zhang Hongbing (张鸿冰). Acta Metall, 1984; 32: 343
13 Chang Hongbing (张鸿冰), Hsu T Y (Xu Zuyao) (徐祖耀). Acta Metall, 1986; 34: 333t
[1] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[2] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[3] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[4] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[5] ZHU Dongming, HE Jiangli, SHI Genhao, WANG Qingfeng. Effect of Welding Heat Input on Microstructure and Impact Toughness of the Simulated CGHAZ in Q500qE Steel[J]. 金属学报, 2022, 58(12): 1581-1588.
[6] JIANG Zhonghua, DU Junyi, WANG Pei, ZHENG Jianneng, LI Dianzhong, LI Yiyi. Mechanism of Improving the Impact Toughness of SA508-3 Steel Used for Nuclear Power by Pre-Transformation of M-A Islands[J]. 金属学报, 2021, 57(7): 891-902.
[7] LIU Feng, WANG Tianle. Precipitation Modeling via the Synergy of Thermodynamics and Kinetics[J]. 金属学报, 2021, 57(1): 55-70.
[8] WANG Zumin,ZHANG An,CHEN Yuanyuan,HUANG Yuan,WANG Jiangyong. Research Progress on Fundamentals and Applications of Metal-Induced Crystallization[J]. 金属学报, 2020, 56(1): 66-82.
[9] Chengming ZHENG, Qingchao TIAN. Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel[J]. 金属学报, 2019, 55(4): 427-435.
[10] Shixin XU, Wei YU, Shujia LI, Kun WANG, Qisong SUN. Effects of Pre-Deformation Temperature on Nanobainite Transformation Kinetics and Microstructure[J]. 金属学报, 2018, 54(8): 1113-1121.
[11] Huidong WU, Goro MIYAMOTO, Zhigang YANG, Chi ZHANG, Hao CHEN, Tadashi FURUHARA. Incomplete Bainite Transformation Accompanied with Cementite Precipitation in Fe-1.5(3.0)%Si-0.4%C Alloys[J]. 金属学报, 2018, 54(3): 367-376.
[12] Xiaofeng HU, Haichang JIANG, Mingjiu ZHAO, Desheng YAN, Shanping LU, Lijian RONG. Microstructure and Mechanical Properties of Welded Joint of a Fe-Cr-Ni-Mo Steel with High-Strength and High-Toughness[J]. 金属学报, 2018, 54(1): 1-10.
[13] Liansheng CHEN, Yue LI, Mingshan ZHANG, Yaqiang TIAN, Xiaoping ZHENG, Yong XU, Shihong ZHANG. Effect of Intercritical Dislocation Multiplication to Mn Partitioning and Microstructure Evolution of Bainite in Low Carbon Steel[J]. 金属学报, 2017, 53(11): 1418-1426.
[14] Xiaolu GUI,Baoxiang ZHANG,Guhui GAO,Ping ZHAO,Bingzhe BAI,Yuqing WENG. FATIGUE BEHAVIOR OF BAINITE/MARTENSITE MULTIPHASE HIGH STRENGTH STEEL TREATEDBY QUENCHING-PARTITIONING-TEMPERING PROCESS[J]. 金属学报, 2016, 52(9): 1036-1044.
[15] Liheng LIU,Chunshan CHE,Gang KONG,Jintang LU,Shuanghong ZHANG. DESTABILIZATION MECHANISM OF Fe-Al INHIBITION LAYER IN Zn-0.2%Al HOT-DIP GALVANIZING COATING AND RELATED THERMODYNAMIC EVALUATION[J]. 金属学报, 2016, 52(5): 614-624.
No Suggested Reading articles found!