Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (2): 125-131    DOI:
Current Issue | Archive | Adv Search |
MICROSTRUCTURE AND PERFORMANCE OF Ni-Hf BRAZING FILLER ALLOY
ZHENG Yunrong;RUAN Zhongci Institute of Aeronautical Materials; Beijing Senior Engineer; Laboratory No.4;Institute of Aeronautical Materials; Beijing 100095
Cite this article: 

ZHENG Yunrong;RUAN Zhongci Institute of Aeronautical Materials; Beijing Senior Engineer; Laboratory No.4;Institute of Aeronautical Materials; Beijing 100095. MICROSTRUCTURE AND PERFORMANCE OF Ni-Hf BRAZING FILLER ALLOY. Acta Metall Sin, 1990, 26(2): 125-131.

Download:  PDF(2453KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In consideration of the envelopment of γ dendrites by the Hf-richmelts, saying brazing by the melts together, at the late period of solidification of thecast Ni-base superalloys containing Hf, a heat of brazing filler alloy composed ofNi-18.6Co-4.5Cr-4.7W-25.6Hf (wt-%) was prepared. This alloy is hypereutectic. γphase is the leading phase in eutectic γ+Ni_5Hf and γ bars are surrounded by Ni_5Hfphase. At the section perpendicular or parallel to the γ growing direction, the eutec-tic morphology is cellular or laminar respectively. The content of Ni_5Hf in thealloy is 68.7 v. -%. The compositions of primary and eutectic Ni_5Hf are very similar.Ni, Co and Hf are the main elements and the solubility of Cr and W in Ni_5Hf isvery low. This alloy is an ideal brazing filler suitable to the directional or singlecrystal superalloys, and the elements are beneficial to superalloys at all. This alloyis of low melting point and of good fluidity. After brazing at 1240℃, 5 min+1190℃, 1h under 10~(-3) Pa vacuum, the microstructure of bond is as same as thatof Hf-bearing superalloy. No more Si and B will be contaminated.
Key words:  Ni-Hf brazing alloy      Hf-bearing Ni-base superalloy      Ni_5Hf phase      brazing     
Received:  18 February 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I2/125

1 郑运荣.金属学报,1986;22:A119
2 郑运荣.焊接学报,1988;9:162
3 Zheng Yunrong, Li Chenggong. In: Duhl D N Maurer G, Antolovich S, Lund C, Reichman S., eds, Superalloys 1988, AIME, 1988: 475
4 Massalski T B, Murray J L, Bennett L H, Baker H. Binary Alloy Phase Diagrams, Vo1. II, Metals Park, Ohio: ASM, 1986: 1300
5 Duvall D S, Owczarski W A, Paulonis D F. Weld J, 1974; 53: 203
6 Zheng Yunrong, Wang Luobao, Li Chenggong. Chin J Met Sci Technol, 1989; 5: 90u
[1] ZHAO Xu,SUN Yuan,HOU Xingyu,ZHANG Hongyu,ZHOU Yizhou,DING Yutian. Effect of Orientation Deviation on Microstructure and Mechanical Properties of Nickel-Based Single Crystal Superalloy Brazing Joints[J]. 金属学报, 2020, 56(2): 171-181.
[2] Xiaoyi ZHANG, Hailong SHANG, Bingyang MA, Rongbin LI, Geyang LI. Brazing of Coated Al Foil Filler to AlN Ceramic[J]. 金属学报, 2018, 54(4): 575-580.
[3] Geliang LIU, Bingyang MA, Hailong SHANG, Fan CHEN, Rongbin LI, Geyang LI. Wettability Improvement and Brazing of Si3N4by Sputtered Al[J]. 金属学报, 2017, 53(12): 1645-1650.
[4] Yuan SUN,Jide LIU,Xingyu HOU,Guanglei WANG,Jinxia YANG,Tao JIN,Yizhou ZHOU. MICROSTRUCTURE EVOLUTION AND INTERFACIAL FORMATION MECHANISM OF WIDE GAP BRAZING OF DD5 SINGLE CRYSTAL SUPERALLOY[J]. 金属学报, 2016, 52(7): 875-882.
[5] Wei FU,Xiaoguo SONG,Long LONG,Jianhang CHAI,Jicai FENG,Guodong WANG. INTERFACIAL MICROSTRUCTURE AND MECHANI-CAL PROPERTIES OF INDIRECT BRAZED GRAPHITE/COPPER JOINT[J]. 金属学报, 2016, 52(6): 734-740.
[6] YANG Hao, HUANG Jihua, CHEN Shuhai, ZHAO Xingke, WANG Qi, LI Dehua. INFLUENCE OF THE COMPOSITION OF Zn-Al FILLER METAL ON THE INTERFACIAL STRUCTURE AND PROPERTY OF Cu/Zn-Al/Al BRAZED JOINT[J]. 金属学报, 2015, 51(3): 364-370.
[7] SUN Yuan, LIU Jide, LIU Zhongming, YANG Jinxia, LI Jinguo,JIN Tao, SUN Xiaofeng. MICROSTRUCTURE EVOLUTION AND MECHANICAL PROPERTIES OF DD5 SINGLE CRYSTAL SUPERALLOY JOINT BRAZED BY Co—BASED FILLER ALLOY[J]. 金属学报, 2013, 49(12): 1581-1589.
[8] ZHANG Qingke, PEI Yinyin, LONG Weimin. INVESTIGATIONS ON FORMATION MECHANISMS OF BRAZING CRACKS AT THE AUSTENITIC STAINLESS STEEL/FILLER METAL BRAZING JOINT INTERFACES[J]. 金属学报, 2013, 49(10): 1177-1184.
[9] QIN Guoliang SU Yuhu WANG Shujun. MICROSTRUCTURES AND PROPERTIES OF PULSED MIG ARC BRAZED–FUSION WELDED JOINT OF Al ALLOY AND GALVANIZED STEEL[J]. 金属学报, 2012, 48(8): 1018-1024.
[10] LIN Sanbao SONG Jianling YANG Chunli MA Guangchao. MICROSTRUCTURE ANALYSIS OF INTERFACIAL LAYER WITH TUNGSTEN INERT GAS WELDING–BRAZING JOINT OF ALUMINUM ALLOY/STAINLESS STEEL[J]. 金属学报, 2009, 45(10): 1211-1216.
[11] QiuYa Zhai; Cunkun Liang; Junping LIU; Qunsheng XUE. Study on Vacuum Brazing of 25Cr3MoA/YG6 Using Cu-based Microcrystalline Brazing Alloy[J]. 金属学报, 2008, 44(9): 1136-1140 .
[12] Wen-Chun JIANG. Finite Element Analysis of Creep for Micro Stainless Steel Plate-fin Heat Exchanger[J]. 金属学报, 2007, 43(5): 539-545 .
[13] . STUDY OF BRAZING ALLOY USED IN BRAZING COMPOSITE ALLOY CLADDING REINFORCED WITH HARD PARTICLES[J]. 金属学报, 2007, 43(4): 433-438 .
[14] XiaoSong Feng. TEMPERATURE FILED SIMULATION OF LASER BRAZING FOR GALVANIZED STEEL SHEETS[J]. 金属学报, 2006, 42(8): 882-886 .
[15] WANG Liduo;WANG Yinghua;LI Wenzhi; LI Hengde (Tsinghua University; Beijing 100084); OKI Takeo (Naguya University; Japan). REACTION BEHAVIOUR OF ZrO_2/Ti INTERFACE IN JOINTING ZIRCONIA CERAMICS AND STAINLESS STEEL 304 WITH Ti FOIL[J]. 金属学报, 1997, 33(7): 756-762.
No Suggested Reading articles found!