Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (2): 120-124    DOI:
Current Issue | Archive | Adv Search |
RELATIONSHIP BETWEEN COMPOSITION UNIFORMITY AND SHAPE COEFFICIENT OF MOLTEN POOL BY LASER ALLOYING
LIANG Yong;ZENG Xiaoyan;TONG Baiyun;SI Zhongyao Institute of Metal Research; Academia Sinica; Shenyang professor;Institute of Metal Research;Academia Sinica;Shenyang 110015
Cite this article: 

LIANG Yong;ZENG Xiaoyan;TONG Baiyun;SI Zhongyao Institute of Metal Research; Academia Sinica; Shenyang professor;Institute of Metal Research;Academia Sinica;Shenyang 110015. RELATIONSHIP BETWEEN COMPOSITION UNIFORMITY AND SHAPE COEFFICIENT OF MOLTEN POOL BY LASER ALLOYING. Acta Metall Sin, 1990, 26(2): 120-124.

Download:  PDF(408KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of the laser processing parameters on the composition unifor-mity and shape coefficient of fusion zone with laser surface alloyed Cr plated onmedium carbon low alloy steel has been studied. It was found that the compositionuniformity depends on the shape coefficient of fusion zone, and the later is a func-tion of both power density and interaction time. If the power density is certain va-lue, it is proportional directly to the interaction time. A complete uniformal moltenpool can be gotten, when the shape coefficient is between 1.6 and 3.0.
Key words:  laser alloying      composition uniformity      shape coefficient of molten pool     
Received:  18 February 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I2/120

1 Chande T, Mazumder J. Metall Trans, 1983; 14B: 181
2 Molian P A. Scr Metall, 1982; 16: 65
3 Christolou G, Steen W M. Laser in Materials Processing, Metals Park, Ohio: ASM, 1982: 116
4 Anthony T R, Cline H E. J Appl Phys, 1977; 48: 3888
5 Chande T, Mazumder J. Appl Phys Lett, 1982; 41: 42
6 Hill J W, Lee M J, Spalding I J. Optics Laser-Technol, 1974; 6: 276S
[1] LI Jianing, GONG Shuili, WANG Juan, SHAN Feihu, LI Huaixue, WU Bing. INFLUENCE OF Cu ON MICROSTRUCTURES AND WEAR RESISTANCE OF STELLITE 12 MATRIX LASER ALLOYING COATINGS ON TA15-2 TITANIUM ALLOY[J]. 金属学报, 2014, 50(5): 547-554.
[2] ZHANG Song, WU Chenliang, WANG Chao, YI Junzhen, ZHANG Chunhua. SYNTHESIS OF LASER HIGH ENTROPY ALLOYING COATING ON THE SURFACE OF SINGLE-ELEMENT Fe BASE ALLOY[J]. 金属学报, 2014, 50(5): 555-560.
[3] WEI Bingqing; ZHANG Jihong; XIONG Zhiwang; LIANG Ji;GAO Zhidong; WU Dehai (Tsinghua University; Beijing 100084). STRENGTHENING STEEL 45 BY BUCKYTUBES UNDER LASER IRRADIATION[J]. 金属学报, 1997, 33(6): 655-659.
[4] WU Ping; ZHOU Changzhi; TANG Xi'nan (Tsinghua Univereity; Beijing)(Manuscript received 11 April;1994). PREPARATION OF WEAR-RESISTANT GRADED METAL-CERAMIC COATING BY LASER-ALLOYING[J]. 金属学报, 1994, 30(23): 508-512.
[5] CHENG YongXing;LI Genfu;YU Shaoluo Shanghai University of Engineering Science Department No.5;Shanghai University of Engineering Science; Shanghai 200051. OBSERVATION ON MICROSTRUCTURE OF LASER MELTED TRANSITION ZONE[J]. 金属学报, 1990, 26(1): 64-68.
[6] Cheng Yongxing;LI Genfu;YU Shaoluo;WANG Huimin Shanghai University of Engineering and technology NO. 11 Institute of China State Shipbuilding Corp.; Shanghai Manuscript received 29 July; 1987; revised manuscript 3 January; 1988. ELECTRON MICROANALYSIS FOR LASER MELTED ZONE IN 45 STEEL WITH Fe-Ni-Cr COATING[J]. 金属学报, 1988, 24(6): 415-418.
No Suggested Reading articles found!