Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (4): 22-26    DOI:
Current Issue | Archive | Adv Search |
GROWTH OF Bi(Pb)-Sr-Ca-Cu-O SUPERCONDUCTING WHISKERS
GE Yunlong;LIU Qingmin;ZHOU Jing;CHANG Xin;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang associate professor
Cite this article: 

GE Yunlong;LIU Qingmin;ZHOU Jing;CHANG Xin;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang associate professor. GROWTH OF Bi(Pb)-Sr-Ca-Cu-O SUPERCONDUCTING WHISKERS. Acta Metall Sin, 1990, 26(4): 22-26.

Download:  PDF(2633KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Amorphous Bi(Pb)-Sr-Ca-Cu-O strips of (1112) and (2212) types weremade by non-equilibrium solidification of melt-quenching method. On the surfaceof glassy strip, the flexible (2212) superconducting whiskers have been obtained at840-850℃ in a stream of O_2 for a long time. The growth and feature of supercon-ducting whiskers were studied in deteil.
Key words:  Bi(Pb)-Sr-Ca-Cu-O superconductor      whisker      non-equilibrium solidification     
Received:  18 April 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I4/22

1 Hikita M, Iwata T, Tajima Y, Katsui A. J Cryst Growth, 1988; 91: 282
2 Ciszek T F, Goral J P, Evans C D, Kotayama-Yoshida H. J Cryst Growth, 1988; 91: 312
3 Takekawa S, Nozaki H, Umezono A, Kosuda K, Kobayashi M. J Cryst Growth, 1988; 92: 687
4 Gazit D, Feigelson R S. J Cryst Growth, 1988; 91: 318
5 Katsui A, Ohtsuka H. J Cryst Growth, 1988; 91: 261
6 Matsubara I, Kageyama H, Tanigawa H, Ogura T, Yamashita H, Kawai T. Jpn J Appl phys, 1989; 28: L1121
7 Komatsu T, Imai K, Sato R, Matusita K, Yamashita T. Jpn J Appl Phys, 1988; 27: L53
[1] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[2] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[3] TIAN Zhihua, ZHANG Peigen, LIU Yushuang, LU Chengjie, DING Jianxiang, SUN Zhengming. Research Progress and Outlook of Metal Whisker Spontaneous Growth on MAX Phase Substrates[J]. 金属学报, 2022, 58(3): 295-310.
[4] Jianqiang REN, Shuhua LIANG, Yihui JIANG, Xiang DU. Research on the Microstructure and Properties of In Situ (TiB2-TiB)/Cu Composites[J]. 金属学报, 2019, 55(1): 126-132.
[5] Yun LI, Lianjie LIU, Xinming LI, Jinfu LI. Solidification of Undercooled Co75B25 Alloy[J]. 金属学报, 2018, 54(8): 1165-1170.
[6] Feng LIU, Xu ZHANG, Yubing ZHANG. Unified Analysis of Non-Equilibrium Solidification and Solid-State Phase Transformations[J]. 金属学报, 2018, 54(5): 701-716.
[7] Yong ZUO, Limin MA, Sihan LIU, Yutian SHU, Fu GUO. WHISKER MITIGATION FOR Sn-BASED Pb-FREE SOLDERS BY POSS ADDITION[J]. 金属学报, 2015, 51(6): 685-692.
[8] LIU Gang, TANG Shawei, HU Jin. EFFECTS OF SINTERING TEMPERATURE OF WHISKER PREFORM ON THE DAMPING PROPERTIES OF BI(OH)3-COATED AL18B4O33 WHISKER-REINFORCED ALUMINUM COMPOSITES[J]. 金属学报, 2014, 50(3): 361-366.
[9] LIU Gang SUN Yali HU Jin ZHOU Ke. DAMPING CAPACITY OF Bi2O3–COATED Al18B4O33 WHISKER REINFORCED Al MATRIX COMPOSITES[J]. 金属学报, 2010, 46(8): 979-983.
[10] HE Hongwen XU Guangchen GUO Fu. FORMATION OF WHISKER AND HILLOCK IN Cu/Sn--58Bi/Cu SOLDERED JOINT DURING ELECTROMIGRATION[J]. 金属学报, 2009, 45(6): 744-748.
[11] HAO Hu SHI Yaowu XIA Zhidong LEI Yongping GUO Fu LI Xiaoyan. CROSS SECTION CHANGING GROWTH PHENOMENON OF Sn WHISKER IN Sn–3.8Ag–0.7Cu–1.0Er LEAD–FREE SOLDER[J]. 金属学报, 2009, 45(2): 199-203.
[12] WU Zhengan; GU Mingyuan; CHEN Yu; ZHANG Gooding (The State Key Laboratory of MMCs; Shanghai Jiaotong University; Shanghai 200030). THE INTERFACE MICROSTRUCTURE OF A B_4C_p +SiC_w/MB15 MAGNESIUM BASED COMPOSITE[J]. 金属学报, 1998, 34(4): 443-448.
[13] XU Gaiying;LI Jianbao;XIE Zhipeng;HUANG Yong (State Key Laboratory of New Ceramics and Fine Processing; Tsinghua University; Beijing 100084). THE PREPARATION OF NbC_x WHISKER[J]. 金属学报, 1998, 34(2): 205-210.
[14] CHEN Weiwu;ZOU Zongshu; WANG Tianming(Northeastern University; Shenyang110006). NEW PROCESS FOR SYNTHETIC SiC WHISKERS BY CVD[J]. 金属学报, 1997, 33(6): 643-649.
[15] CUI Chunxiang; WU Renjie; YANG Chunsheng(Shanghai Jiaotong University.Shanghai 200030)(Manuscript received 1 995-07- 1 7; in revised form 1 995-10-04). IN SITU FORMATION AND DISTRIBUTION OF TiC WHISKERS IN TiC_w-AlN_p/ AI COMPOSITE[J]. 金属学报, 1996, 32(3): 323-327.
No Suggested Reading articles found!