| SUBSTRUCTURAL AND CRYSTALLOGRAPHIC FEATURES OF LOWER BAINITE |
| SUN Jialin Kunming Institute of Technology; KANG Mokuang Northwestern Polytechnical University; Xi'an |
|
Cite this article:
SUN Jialin Kunming Institute of Technology; KANG Mokuang Northwestern Polytechnical University; Xi'an. SUBSTRUCTURAL AND CRYSTALLOGRAPHIC FEATURES OF LOWER BAINITE. Acta Metall Sin, 1991, 27(3): 72-76.
|
|
|
Abstract Based on the TEM analysis of substructures of lower bainite in twosteels containing Si, the lattice invariant shear elements were determined and a plasticaccommodation double-shear model was proposed. The theorotical predictions aboutcrystallography given by the model are in good agreement with the experimental da-ta for the steels tested.
|
|
Received: 18 March 1991
|
1 Bowles J S, Kennon N F. J Aust Inst Met, 1960; 5: 106 2 Srinivasan G R, Wayman C M. Acta Metall, 1968; 16: 609, 621 3 Ross N D H, Crocker A G. Acta Metall, 1970; 18: 405 4 Ohmori Y. Trans Iron Steel Inst Jpn, 1971; 11: 95 5 Hoekstra S. Acta Metall, 1980; 28: 507 6 孙加林.西北工业大学博士学位论文,1989 7 Sandvik B P J. Metall Trans, 1982; 13A: 777 8 Sandvik B P J, Wayman C M. Metall Trans, 1983; 14A: 809 9 Wechsler M S, Lieberman D S, Read T A. Trans AIME, 1953; 197: 1503 10 Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129, 138, 224 11 Sandvik B P J, Wayman C M. Metall Trans, 1983; 14A: 2469 12 康沫狂,杨思品,管敦惠.纲中贝氏体,上海,上海科学技术出版社,1990 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|