Acta Metall Sin  1991, Vol. 27 Issue (5): 130-135    DOI:
Current Issue | Archive | Adv Search |
X-RAY PHOTOELECTRON SPECTROSCOPY OF HIGH Tc SUPERCONDUCTOR YBa_2 Cu_3 O_(7-x)
TIAN Lu;WANG Wenhao;GONG Yandong;SUN Yuzhen;LIN Shuzhi Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

TIAN Lu;WANG Wenhao;GONG Yandong;SUN Yuzhen;LIN Shuzhi Institute of Metal Research; Academia Sinica; Shenyang. X-RAY PHOTOELECTRON SPECTROSCOPY OF HIGH Tc SUPERCONDUCTOR YBa_2 Cu_3 O_(7-x). Acta Metall Sin, 1991, 27(5): 130-135.

Download:  PDF(518KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The XPS spectra of superconducting (123-orthorhombic structure) and non-superconducting (123-tetragonal structure) YBa_2Cu_3O_(7-x). ceramics were obtained at room temperature and 130 K in RIBER LAS 3000 surface analysis system, in which a sample cooling stage and a surface cleaning scraper, both made by the authors'own, were installed. No evidence of Cu~(3+) was found. The O1s shows double lines.They are attributed to O1 and O4 with higher binding energy and to O2 and O3 with lower binding energy respectively, and it was confirmed by calculation of SW-X_α method. The differences and changes in valence states of Y, Ba, Cu and O in both samples were discussed.
Key words:  YBaCuO      superconductor      low temperature      XPS     
Received:  18 May 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I5/130

1 Capponi J J, Chaillout C, Hewat A W, Leiay P, Maresio M, Nguyen N, Raveau B, Tholeace T L, Teurnier R. Eur Phys Lett, 1989; 3: 1310
2 Wang Wenhao, Tian Lu, Gong Yandong, Sun Yuzhen. Surf Sci, 1989; 213: 303
3 江晓平.低温物理学报,1987;9:192
4 Steiner P, Kinsinger V, Sander I, Siegwart B, Hufner S, Politis C, Hoppe R, Muller H P. Z Phys, 1987; B67: 497
5 Bianconi A, Congiu A, Castellano C, De Santis M, De Logu P, Gargano A, Giorgi R. Solid State Commun, 1987; 63: 1135
6 Anderson P W. In: Broglia R A, Schrieffer J R eds., Proc of the E. Fermi Inter. Summer School of Physics on Frontiers and Borderline in Many Particle Physics, Varenna, Italy, 1987, Amsterdam: North-Holland, 1987: 156
7 Fujimori A, Takayama-Muromachi E, Uchida Y, Okai B. Phys Rev, 1987; B35: 8814
8 Feil H. Solid State Commun, 1989; 69: 245
9 Larsson S. Chem Phys Lett, 1976; 40: 362
10 McIntyre N S, Cook M G. Anal Chem, 1975; 47: 2208
11 Beno M A, Soderholm L, Capone D W, Hinks D G, Jogensen J D, Grace J D, Schuller I K, Segre C U, Zhang K. Appl Phys Lett, 1987; 51: 57
12 Wagner C D, Riggs W M, Davis L E, Moulder J F. In: Mullerber G E ed, Handbook of X Ray Photoelectron Spectroscopy, USA: Perkin Elmer Co., 1979
[1] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[2] WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei. Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K[J]. 金属学报, 2023, 59(2): 277-288.
[3] Hanchen FENG,Xuegang MIN,Dasheng WEI,Lichu ZHOU,Shiyun CUI,Feng FANG. Effect of Low Temperature Annealing on Microstructure and Mechanical Properties of Ultra-Heavy Cold-DrawnPearlitic Steel Wires[J]. 金属学报, 2019, 55(5): 585-592.
[4] QIN Jiayu, LI Xiaoqiang, JIN Peipeng, WANG Jinhui, ZHU Yunpeng. Microstructure and Mechanical Properties of Carbon Nanotubes (CNTs) Reinforced AZ91 Matrix Composite[J]. 金属学报, 2019, 55(12): 1537-1543.
[5] SONG Guihong,LI Guipeng,LIU Qiannan,DU Hao,HU Fang. Microstructure and Electric Conductance of Mg2(Sn, Si) Thin Films by Sputtering[J]. 金属学报, 2019, 55(11): 1469-1476.
[6] Yubin DU, Xiaofeng HU, Haichang JIANG, Desheng YAN, Lijian RONG. Effect of Tempering Time on Carbide Evolution and Mechanical Properties in a Fe-Cr-Ni-Mo High-Strength Steel[J]. 金属学报, 2018, 54(1): 11-20.
[7] Liming DONG,Li YANG,Jun DAI,Yu ZHANG,Xuelin WANG,Chengjia SHANG. Effect of Mn, Ni, Mo Contents on Microstructure Transition and Low Temperature Toughness of Weld Metal for K65 Hot Bending Pipe[J]. 金属学报, 2017, 53(6): 657-668.
[8] Chengxu HE,Fuyao YANG,Guochun YAN,Li MENG,Guang MA,Xin CHEN,Weimin MAO. EFFECT OF NORMALIZING ON TEXTURES OF THIN-GAUGE GRAIN-ORIENTED SILICON STEEL[J]. 金属学报, 2016, 52(9): 1063-1069.
[9] Xuelin WANG,Liming DONG,Weiwei YANG,Yu ZHANG,Xuemin WANG,Chengjia SHANG. EFFECT OF Mn, Ni, Mo PROPORTION ON MICRO-STRUCTURE AND MECHANICAL PROPERTIESOF WELD METAL OF K65 PIPELINE STEEL[J]. 金属学报, 2016, 52(6): 649-660.
[10] Changjun WANG,Jianxiong LIANG,Zhenbao LIU,Zhiyong YANG,Xinjun SUN,Qilong YONG. EFFECT OF METASTABLE AUSTENITE ON MECHANI-CAL PROPERTY AND MECHANISM IN CRYOGENICSTEEL APPLIED IN OCEANEERING[J]. 金属学报, 2016, 52(4): 385-393.
[11] Zhenjia XIE,Chengjia SHANG,Wenhao ZHOU,Binbin WU. EFFECT OF RETAINED AUSTENITE ON DUCTILITY AND TOUGHNESS OF A LOW ALLOYED MULTI-PHASE STEEL[J]. 金属学报, 2016, 52(2): 224-232.
[12] Dongsong RONG,Yong JIANG,Jianming GONG. EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(12): 1516-1522.
[13] GAO Guhui, GUI Xiaolu, AN Baifeng, TAN Zhunli, BAI Bingzhe, WENG Yuqing. EFFECT OF FINISH COOLING TEMPERATURE ON MICROSTRUCTURE AND LOW TEMPERATURE TOUGHNESS OF Mn-SERIES ULTRA-LOW CARBON HIGH STRENGTH LOW ALLOYED STEEL[J]. 金属学报, 2015, 51(1): 21-30.
[14] WANG Yanfei, GONG Jianming, RONG Dongsong, GAO Feng. MEASUREMENT AND CALCULATION OF CARBON CONCENTRATION AND DIFFUSION-INDUCED STRESS IN STAINLESS STEEL AFTER LOW TEMPERATURE GAS CARBURIZING[J]. 金属学报, 2014, 50(4): 409-414.
[15] ZHAO Dongqing, ZHOU Jixue, LIU Yunteng, DONG Xuguang, WANG Jing, YANG Yuansheng. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Mg-4Zn-2Al-2Sn ALLOYS EXTRUDED AT LOW TEMPERATURES[J]. 金属学报, 2014, 50(1): 41-48.
No Suggested Reading articles found!